| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
|
Oxford Polymers 10GF 10% Glass Fiber Filled Polycarbonate for Injection Molding
10% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers.
|
|||
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
|
Oxford Polymers Polysulfone PSF P170-64170 White PSU
Product Description: Polysulfone injection molding grade, precolored white Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Continuous use up to 300(f)Informatio..
|
|||
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
|
Quadrant EPP Nylatron® GSM Blue Nylon, Cast Oil & MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
|
Polymer Resources PPX-G10 Modified-PPO, 10% Glass Reinforced
Modified-Polyphenylene Oxide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
|
Polymer Resources NY66-MD02-[color]-H Nylon, 2% Molybdenum disulfide for lubrication and wear, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
|
Quadrant EPP Quadrant LSG PSU, Extruded, Unfilled, Polysulfone (ASTM Product Data Sheet) |
|||
| Flexural Strength | 103 - 117 MPa | 15000 - 17000 psi | ASTM D790 |
|
Mar-Bal MB3000-15 Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
|
|||
| Flexural Strength | 103 MPa | 15000 psi | 2.0 in/min; ASTM D790 |
|
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate
High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc.
|
|||
| Flexural Strength |
103
MPa @Thickness 3.17 mm, Temperature 22.8 °C |
15000
psi @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D790 |
|
MRC Polymers NAXALOYâ„¢ 793A3 GF10 PC and Polyester Blend, 10% Glass Fiber Filled
793 GF10 is available in natural and custom colors, internal and external lubricants, UV stabilizer and other modifications.Information provided by MRC Polymers Inc.
|
|||
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
|
Techmer ES HiFill® PA11 GB7 HS L 7% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 7% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by T..
|
|||
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
|
Techmer ES HiFill® PA4/6 HS LBK
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackTPCI# 9651150Information provided by TP Composites, Inc.
|
|||
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
|
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated
Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex
|
|||
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
|
Plastics Group Polifil® 930L Nylon 6 (DAM)
Polifil® NYLON 6 provides superior strength and rigidity with electrical resistance and surface lubricity.Applications: AutomotiveHousingsBearingsAppliances Standard processing techniques are appli..
|
|||
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
|
Chase Plastics CP Pryme® NN300HSL (DAM) Nylon 66 (Utility Grade), Heat Stabilized, Internally Lubricated
Information provided by Chase Plastics.
|
|||
| Flexural Strength | 103 MPa | 15000 psi | perpendicular |
|
Carlisle 201LL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
|
|||
| Flexural Strength | 103 MPa | 15000 psi | Crosswise; ASTM D790 |
|
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8"
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
|
|||
| Flexural Strength | 103 MPa | 15000 psi | ASTM D570 |
|
Solvay Specialty Polymers Xydar® M-345 Liquid Crystal Polymer, 45% Mineral Filled
(discontinued **)
XYDAR M-345 Liquid Crystal Polymer (LCP) is a 45% mineral-filled injection molding grade with exceptional moldability. XYDAR M-345 resin can fill very thin walls over long flow lengths with little o..
|
|||