| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC (Asia Pacific)
LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
PolyOne Stat-Tech™ PS-18CF/000 CM Black Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinu
Preliminary Data SheetDescription/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized
Nylon 6, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized
Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific)
LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (DAM)
(discontinued **)
Information provided by Ravago.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES
LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing 30% Glass Fiber, 15% PTFE. Added featurs of this material is: Wear Resistant.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
|
SABIC Innovative Plastics ULTEM 2312 PEI (Asia Pacific)
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS (Asia Pacific)
LNP* Stat-kon* AX02747 is a compound based on Acrylonitrile Butadiene Styrene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D 790 |
|
SABIC Innovative Plastics LNP Stat-kon OE002 PPS
LNP* Stat-kon* OE002 is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP ..
|
|||
| Flexural Strength | 179 MPa | 26000 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific)
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P..
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP STAT-KON ZE004 MODIFIED POLYPHENYLENE (Asia Pacific)
LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP STAT-KON ZE004 PPO
LNP* STAT-KON* ZE004 is a compound based on PPO resin containing 20% Carbon Fiber. Added feature of this grade includes: Electrically Conductive.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
Techmer ES HiFill® PPS 0231 B LE
Availability: North AmericaForms: PelletsFeatures: High Density and Low ExtractablesAppearance: OpaqueInformation provided by TP Composites, Inc.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP VERTON MV008S PP
LNP VERTON* MV008S is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP VERTON MV008SU PP (Europe-Africa-Middle East)
LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized, UV-Stabilized.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP PX92248 PA 6
LNP* THERMOCOMP* PX92248 is a compound based on Nylon 6 resin containing Proprietary Filler(s).
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP RFZ349XC PA 66 (Asia Pacific)
LNP* THERMOCOMP* RFZ349XC is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Flame Retardant.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP RX06420 PA 66 (Asia Pacific)
LNP* Thermocomp* RX06420 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Low Extractible, Mold Release.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
Chase Plastics CP Pryme® NN113L (Dry) Nylon 66, 13% Glass Fiber Reinforced, Lubricated
Features: Good chemical resistanceGrease resistantLubricatedOil resistantHigh rigiditySolvent resistantHigh tensile strengthForm: PelletsInformation provided by Chase Plastics.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
Chase Plastics CP Pryme® PC330GR Polycarbonate (Utility Grade), 30% Glass Fiber Reinforced, Mold Release
Information provided by Chase Plastics.
|
|||
| Flexural Strength | 179 - 214 MPa | 26000 - 31000 psi | |
|
Bulk Molding Compounds BMC 695 Vinyl Ester Molding Compound
BMC 695 vinyl ester molding compound is a mineral filled glass fiber-reinforced vinyl ester compound suitable for compression and injection molding It is characterized by good moldability, oil and s..
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP STAT-KON OE002 PPS (Asia Pacific)
LNP* Stat-kon* OE002 is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
Techmer ES HiFill FR® PA6/6 GF25 FR 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightUL File Number: E157318TPCI# 9085101Information provided by TP Composites, Inc.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP EFL34HL PEI
LNP LUBRICOMP* EFL34HL is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable.
|
|||
| Flexural Strength | 179 MPa | 26000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC
LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated.
|
|||