Mechanical Properties Metric English Comments
Flexural Strength 95.0 - 130 MPa
13800 - 18900 psi
ASTM D790
Prodways PLASTCure Model 300 3D Printing Polymer
Good mechanical properties.Broad range of dental model applications.Information provided by Genistar.
Flexural Strength 110 - 130 MPa
16000 - 18900 psi
ASTM D790-03
Proto3000 Objet RGD525 High Temperature Prototyping Polymer
Information provided by Proto3000 for their protoyping engineering services.
Flexural Strength 100 - 130 MPa
14500 - 18900 psi
Compression; ISO 178
Raschig Group DECAL® 666/8 Phenolic
Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod..
Flexural Strength 100 - 130 MPa
14500 - 18900 psi
Injection; ISO 178
Raschig Group MELOPAS® 2010 MF Melamine
Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav..
Flexural Strength 90.0 - 130 MPa
13100 - 18900 psi
Injection; ISO 178
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Flexural Strength 100 - 130 MPa
14500 - 18900 psi
Injection; ISO 178
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
Flexural Strength 100 - 130 MPa
14500 - 18900 psi
Injection; ISO 178
Raschig Group MELOPLAS® 181 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc..
Flexural Strength 100 - 130 MPa
14500 - 18900 psi
Injection; ISO 178
Raschig Group MELOPLAS® 181.5 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis..
Flexural Strength 100 - 130 MPa
14500 - 18900 psi
Compression; ISO 178
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Flexural Strength 110 - 130 MPa
16000 - 18900 psi
Injection; ISO 178
Raschig Group MELOPLAS® 3025 MF
Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu..
Flexural Strength 110 - 130 MPa
16000 - 18900 psi
Injection; ISO 178
Raschig Group RALUPOL® 4806 UP
Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80..
Flexural Strength 85.0 - 130 MPa
12300 - 18900 psi
Compression; ISO 178
Raschig Group RALUPOL® 5000 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all..
Flexural Strength 100 - 130 MPa
14500 - 18900 psi
DIN 54352
Schwartz Technical Plastics LAMINEX® 2010 Cotton Fabric, Phenolic Resin Impregnated, Fine
Application: slippers, inserts for coupling boxes, rollneck bearingsInformation provided by Schwartz Technical Plastics GmbH
Flexural Strength 110 - 130 MPa
16000 - 18900 psi
At Rupture; ISO 178
Vyncolit 4221 XB Novolac Phenolic
Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group
Flexural Strength 120 - 130 MPa
17400 - 18900 psi
At Rupture; ISO 178
Vyncolit 4451 XB Novolac Phenolic
Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a..
Flexural Strength 100 - 130 MPa
14500 - 18900 psi
Injection; ISO 178
Raschig Group MELOPLAS® 180 MF
Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing ..
Flexural Strength 110 - 130 MPa
16000 - 18900 psi
Injection; ISO 178
Raschig Group 5557 DAP  (discontinued **)
Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h..
Flexural Strength 100 - 130 MPa
14500 - 18900 psi
ISO 178
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound
Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat..