Polymer Property : Flexural Strength = 20000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Strength 124 - 138 MPa
18000 - 20000 psi
ASTM D790
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Flexural Strength 103 - 138 MPa
15000 - 20000 psi
ASTM D790
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon
Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau..
Flexural Strength 103 - 138 MPa
15000 - 20000 psi
Bulk Molding Compounds BMC 2270 Mineral Filled, Glass Reinforced Polyester
BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength a..
Flexural Strength 103 - 138 MPa
15000 - 20000 psi
Bulk Molding Compounds BMC 3001H Mineral Filled Alkyd
BMC 3001H molding compound is a mineral filled, glass-fiber reinforced alkyd compound suitable for compression and transfer molding. Because of its soft flow, it is also used extensively in cold spu..
Flexural Strength 124 - 138 MPa
18000 - 20000 psi
Bulk Molding Compounds BMC 5209 Mineral Filled, Glass Reinforced Polyester
BMC 5209 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex..
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Bulk Molding Compounds BMC 5436 Mineral Filled, Glass Reinforced Polyester
BMC 5436 molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda..
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium ..
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Bulk Molding Compounds BMC 600LS Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 600LS molding compound is a low-shrink, Mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose materia..
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit..
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda..
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Bulk Molding Compounds BMC 605LS Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 605LS molding compound is a low-shrink, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good mol..
Flexural Strength 103 - 138 MPa
15000 - 20000 psi
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext..
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Bulk Molding Compounds BMC 6241 Glass Fiber Reinforced Compound
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availabl..
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab..
Flexural Strength 96.5 - 138 MPa
14000 - 20000 psi
Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant
BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs,..
Flexural Strength 117 - 138 MPa
17000 - 20000 psi
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound
BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a..
Flexural Strength 103 - 138 MPa
15000 - 20000 psi
Bulk Molding Compounds BMC 880 Medium Strength Molding Compound
BMC 880 is a medium strength, low shrink molding compound designed for outdoor applications. This material is UL Listed 94-V0/5V and is UL approved for outdoor use. It can be supplied in bulk or ext..
Flexural Strength 124 - 138 MPa
18000 - 20000 psi
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound
BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. ..
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Bulk Molding Compounds BMC T9 General Purpose Molding Compound
BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9..
Flexural Strength 96.5 - 138 MPa
14000 - 20000 psi
Bulk Molding Compounds BMC 1000 Thermoset Polyester, Food Grade
BMC 1000 is a general purpose, food contact grade, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. As with all other BMC, Inc. compounds, ..
Flexural Strength 103 - 138 MPa
15000 - 20000 psi
Bulk Molding Compounds BMC 1901 Mineral Filled Alkyd
BMC 1901 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression transfer molding. It is a general purpose with medium impact strength and good overall e..
Flexural Strength 103 - 138 MPa
15000 - 20000 psi
Bulk Molding Compounds BMC 2201 Mineral Filled Alkyd
BMC 2201 molding compound is a mineral filled, glass-fiber-and nylon-floc reinforced alkyd compound suitable for compression and transfer molding. It was developed for applications requiring better ..
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester
BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium..
Flexural Strength 96.5 - 138 MPa
14000 - 20000 psi
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade
BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings.
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Bulk Molding Compounds BMC 5307 Mineral Filled, Glass Reinforced Polyester
BMC 5307 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a medium impact material produced in ..
Flexural Strength 110 - 138 MPa
16000 - 20000 psi
Bulk Molding Compounds BMC 605 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 605 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, medi..
Flexural Strength 103 - 138 MPa
15000 - 20000 psi
Bulk Molding Compounds BMC 6605A Polyester Molding Compound
Flexural Strength 117 - 138 MPa
17000 - 20000 psi
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound
BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar..
Flexural Strength 124 - 138 MPa
18000 - 20000 psi
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound
BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty..