| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 270 MPa | 39200 psi | STN EN ISO 178 |
|
Plastcom SLOVAMID 66 GF 35 Polyamide 66, 35% Glass Fiber
FeaturesChemically reinforced with 35% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | |
|
Plastcom SLOVASTER® E GF 30 PBT, 30% glass fibre
FeaturesPET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Nilit FRIANYL A63 W-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Strength | <= 270 MPa | <= 39200 psi | ISO 178 |
|
Polykemi AB SCANAMID 66 A12^ F35 NH9 Nylon 66, Glass Fiber Reinforced, Flame Retardant, Halogen Free
Information provided by Polykemi AB
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ASTM D790 |
|
Premix Premi-Glas® 1281-47 VE SMC
Description: Premi-Glas® 1281-47 VE is a sheet molding compound.Market: StructuralInformation provided by Premix.
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
DSM Akulon® K-FG6 (Dry) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
DSM Akulon® K-FHG6 (Dry) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | |
|
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | 5 mm/min; ISO 178 |
|
Gromax BFG30-B103N1 Nylon 6 33% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Flexural Strength | 270 MPa | 39200 psi | 5 mm/min; ISO 178 |
|
Gromax BFG30-FH00B2 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Flexural Strength | 270 MPa | 39200 psi | |
|
Lehmann & Voss LUVOCOM® 1-0889-2 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL16 PA 66 (Asia Pacific)
LNP LUBRICOMP* RFL16 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Strength | 270 MPa | 39200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP STAT-KON EX11318C PEI (Asia Pacific)
LNP* Stat-Kon* EX11318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178-93 |
|
Wellman Wellamid® GF33A099-HRN Nylon 66, 33% Glass Reinforced, Hydrolysis Resistant
All information provided by Wellman Engineered Resins.
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178-93 |
|
Wellman Wellamid® GFX1743-BK1(PTFE) 45% Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6
Description: Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6Information provided by Wellman.
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178-93 |
|
Wellman Wellamid® WE1410 43% Glass Fiber Reinforced Nylon 66
Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman.
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
DSM Akulon® Ultraflow™ K-FG6 Nylon 6-30% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | dry; ISO 178 |
|
DSM EcoPaXX® Q-X07209 PA410-I-GF40
% Glass Reinforced, Impact Modified
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Eurotec® Tecomid® NA40 GR30 NL RT PA 6.6 30% glass fiber reinforced, very low friction and wear
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Flexural Strength | <= 270 MPa | <= 39200 psi | ISO 178 |
|
Azoty Tarnow™ Tarnamid® T-27 CF40 Polyamide 6 40% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry)
Information provided by BASF
|
|||
| Flexural Strength | 270 MPa | 39200 psi | 2 [mm/min]; ISO 178 |
|
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ASTM D790 |
|
Solvay TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY
Description: Polyamid 66, 30% glass fiber reinforce, for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2411GF6 used in all sectors of industry, offering an excellent com..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **)
Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope..
|
|||