| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 190 MPa | 27600 psi | ASTM D-790 |
|
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% long glass fiber reinforcementInformation provided by PlastiCom..
|
|||
| Flexural Strength | 190 MPa | 27600 psi | |
|
Plastcom SLOVAMID 6 NG GF 20 HLS PA6, 20% glass fibre, combined stability
FeaturesPA 6 for injection moulding, chemically reinforced with 20% glass fibre, heat stabilized and weather stabilized. Stabilized against hydrolysis. Good surface finisch.Packaging, transport, sto..
|
|||
| Flexural Strength | <= 190 MPa | <= 27600 psi | ISO 178 |
|
Polykemi AB SCANMID 6 B12^ QF2515 Nylon 6, Glass Fiber and Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Strength | 190 MPa | 27600 psi | ISO 178 |
|
Idemitsu Kosan Xarec® EA 528 SPS, 30% Glass Filled
(discontinued **)
Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications
|
|||
| Flexural Strength | 190 MPa | 27600 psi | ISO 178 |
|
Nilit FRIANYL B63 GV15 Nylon 6 for injection molding, 15% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Strength | 190 MPa | 27600 psi | |
|
Lehmann & Voss LUVOCOM® 1105-7776 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Emergency running pro..
|
|||
| Flexural Strength | 190 MPa | 27600 psi | |
|
Lehmann & Voss LUVOCOM® 3-7234-1 Polyamide 6, with carbon fiber, electrically conducting
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressAntistatic.Handles, levers, rollers, body parts.Information provided by L..
|
|||
| Flexural Strength | 190 MPa | 27600 psi | 2mm/min; ASTM D790 |
|
Kingfa PBT-G30 30% Glass Fiber Reinforced PBT
Features:Good size stabilityHigh mechanical propertiesHigh heat resistanceExcellent balance propertiesApplications:Injection moldingApplication partsAuto handleDoor latchE & E partsInformation Provi..
|
|||
| Flexural Strength |
190
MPa <br>@Temperature 22.0 °C
|
27600
psi <br>@Temperature 71.6 °F
|
25 mm wide 100 mm long, flat samples; ISO 14125 |
|
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP
SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain..
|
|||
| Flexural Strength | 190 MPa | 27600 psi | ASTM D790 |
|
Mitsui Arlenâ„¢ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Flexural Strength | 190 MPa | 27600 psi | |
|
Lehmann & Voss LUVOCOM® 1105/GF/20/EM/BK PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
|
|||
| Flexural Strength | 190 MPa | 27600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East)
VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo..
|
|||
| Flexural Strength | 190 MPa | 27600 psi | GB/T 9341-2008 |
|
Sichuan Deyang Haton® hGR20 Polyphenylene Sulfide, Glass Fiber Reinforced
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD
|
|||
| Flexural Strength | 190 MPa | 27600 psi | ASTM D790 |
|
SABIC Innovative Plastics ULTEM JD4901 PEI (Asia Pacific) |
|||
| Flexural Strength | 190 MPa | 27600 psi | ASTM D790 |
|
Polyram PlusTek PA301G3 Nylon 6.6, Heat Stabilized, 15% Glass Fiber
Heat stabilized, 15% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Strength | 190 MPa | 27600 psi | ISO 178-93 |
|
Wellman Wellamid® MRGF25/25 22H-GY1 Nylon 66, 25% Mineral and 25% Glass Reinforced
All information provided by Wellman Engineered Resins.
|
|||
| Flexural Strength | 190 MPa | 27600 psi | ISO 178-93 |
|
Wellman Wellpet® GF100-N1 30% Glass Fiber Reinforced, Natural PET
Description: Glass Fiber Reinforced, Natural PETInformation provided by Wellman.
|
|||
| Flexural Strength | 190 MPa | 27600 psi | ASTM D790, ISO 178 |
|
EPICHEM Epiter PBT GF 30 Polybutylene Terephthalate, 30% Glass
Characteristics: 30% glass fibre filled
|
|||
| Flexural Strength | 190 MPa | 27600 psi | 2 mm/min; ISO 178 |
|
Eurostar Staramide AG4K PA66, 20% Glass Filled, Injection Molded
AG4K is a Heat and Hydrolytically Stabilized, 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
|
|||
| Flexural Strength | 190 MPa | 27600 psi | 2 mm/min; ISO 178 |
|
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded
BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Flexural Strength | 190 MPa | 27600 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, Conditioned
Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:..
|
|||
| Flexural Strength | 190 MPa | 27600 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, Conditioned
Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
|
|||
| Flexural Strength | 190 MPa | 27600 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, Conditioned
Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete..
|
|||
| Flexural Strength | 190 MPa | 27600 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Conditioned
Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys..
|
|||
| Flexural Strength | 190 MPa | 27600 psi | ASTM D790 |
|
Beijing Chemical Industry KAIFA® 2030 PET Resin
High mechanical strength, Creep resistant, Low frictionInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||