| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | <= 280 MPa | <= 40600 psi | ISO 178 |
|
Polykemi AB SCANMID 6 B11^ F45 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Strength | <= 280 MPa | <= 40600 psi | ISO 178 |
|
Polykemi AB SCANMID 6 B12^ F45 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Strength |
280
MPa <br>@Temperature 23.0 °C
|
40600
psi <br>@Temperature 73.4 °F
|
DAM; ISO 178 |
|
DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTNFE350038 BK083 is a 33% glass reinforced, heat stabilized, lubricated, hydrolysis resistant high performance polyamide resin, developed for improved structural performance. It is also a P..
|
|||
| Flexural Strength | >= 280 MPa | >= 40600 psi | |
|
MarkeTech AN 160 Aluminum Nitride Ceramic Substrate, 99% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ..
|
|||
| Flexural Strength |
280
MPa <br>@Temperature 22.0 °C
|
40600
psi <br>@Temperature 71.6 °F
|
25 mm wide 100 mm long, flat samples; ISO 14125 |
|
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP
SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re..
|
|||
| Flexural Strength | 280 MPa | 40600 psi | |
|
Lehmann & Voss LUVOCOM® 1105/CF/15 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Flexural Strength | 280 MPa | 40600 psi | ASTM D790 |
|
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off..
|
|||
| Flexural Strength | 280 MPa | 40600 psi | ISO 178 |
|
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA), 33% Glass Fiber
Amodel® A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment...
|
|||
| Flexural Strength | 280 MPa | 40600 psi | ISO 178 |
|
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s..
|
|||
| Flexural Strength | 280 MPa | 40600 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA6.10 (Europe-Africa-Middle East)
LNP * THERMOCOMP* QC006 is a compound based on PA610 resin containing Carbon Fiber. Added features include; Electrically Conductive.
|
|||
| Flexural Strength | 280 MPa | 40600 psi | 2 mm/min; ISO 178 |
|
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber
SAXAMID 226F6T3 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It shows its high mechanical strength over a long period and is able to perform at higher..
|
|||
| Flexural Strength | 280 MPa | 40600 psi | ASTM C1161 |
|
M Cubed Technologies RBBC-751 Reaction Bonded Boron Carbide
Reaction-bonded boron carbide for extreme wear environments. Can be cast into very large components (greater than 4 ft. square)Information provided by M Cubed Technologies, Inc.
|
|||
| Flexural Strength | 280 MPa | 40600 psi | ASTM D790 |
|
Polyram PlusTek PA301G7 Nylon 6.6, Heat Stabilized 35% Glass Fiber
Heat stabilized 35% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Strength | 280 MPa | 40600 psi | ISO 178 |
|
Polyram PlusTek PA4501G6 Nylon 66, 30% Glass Fiber Reinforced, Low Friction
30% Glass fiber reinforced Nylon 66 for low friction applications.Information provided by Polyram.
|
|||
| Flexural Strength | 280 MPa | 40600 psi | ASTM D790 |
|
Toyobo VYLOPET® EMC355 Injection Molding Polyester Resin, Glass Reinforced
Applications: HousingsBracketsGear casesFeatures: High RigidityGlass fiber reinforcementInformation provided by Toyobo.
|
|||
| Flexural Strength | 280 MPa | 40600 psi | dry; ISO 178 |
|
DSM Novamid® 1017GH33 BK701 PA6-GF33
33% Glass Reinforced, Heat Stabilized, Injection Molding
|
|||
| Flexural Strength | 280 MPa | 40600 psi | DAM; ISO 178 |
|
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66
(Unverified Data**)
33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
|
|||
| Flexural Strength | 280 MPa | 40600 psi | 2 mm/min; ISO 178 |
|
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding
Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Flexural Strength | 280 MPa | 40600 psi | 2 mm/min; ISO 178 |
|
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded
Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Flexural Strength | >= 280 MPa | >= 40600 psi | cold bending |
|
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain)
LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good ..
|
|||
| Flexural Strength | 280 MPa | 40600 psi | 2 mm/min; ISO 178 |
|
Eurostar Staramide PF007 PA6, 35% Glass Fiber Filled, Injection Molded
Staramide PF007 is a 35% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Flexural Strength | 280 MPa | 40600 psi | at max force; ISO 178 |
|
BASF Ultramid® B3WG7 BK 00564 30% Glass Filled PA6 (Dry)
Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF
|
|||
| Flexural Strength | >= 280 MPa | >= 40600 psi | cold bending |
|
China-Yixing Longly Refractories 75 Alumina Ceramic
LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, ..
|
|||
| Flexural Strength | 280 MPa | 40600 psi | ISO 178 |
|
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits:..
|
|||