| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 290 MPa | 42100 psi | |
|
Plastcom SLOVAMID 66 GF 40 PA66, 40% glass fibre
FeaturesChemically reinforced with 40% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
|
Niche Polymer PA66GF43BK Nylon 66, 43% Glass Fiber Filled
Information provided by Niche Polymer
|
|||
| Flexural Strength | <= 290 MPa | <= 42100 psi | ISO 178 |
|
Polykemi AB SCANMID 6 B11^ F50 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Strength | <= 290 MPa | <= 42100 psi | ISO 178 |
|
Polykemi AB SCANMID 6 B12^ F50 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Strength | 290 MPa | 42100 psi | |
|
Plastcom SLOVAMID 6 GF 50 LTS PA6, 50% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
|
|||
| Flexural Strength | 290 MPa | 42100 psi | |
|
Lehmann & Voss LUVOCOM® 19-7277 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
|
Grupo Repol Dinalon® A1S25 G45 H PA66 45% Glass Fiber, Heat Stabilized
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
|
|||
| Flexural Strength | 290 MPa | 42100 psi | |
|
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c..
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
|
Solvay TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Description: TECHNYL® A 218 V30 Black 34 NG-K is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: Thi..
|
|||
| Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
|
Techmer ES HiFill® PA6 GF50 HS L 50% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizerInformati..
|
|||
| Flexural Strength | 290 MPa | 42100 psi | 2 mm/min; ISO 178 |
|
Sax Polymers SAXAMID 226F10 Nylon 6.6, 50% Glass Fiber
SAXAMID 226F10 is a polyamide 6.6 injection-molding-grade reinforced with 50% glass fibers. It has high mechanical strength.Information provided by SAX Polymers
|
|||
| Flexural Strength | 290 MPa | 42100 psi | 2 mm/min; ISO 178 |
|
Sax Polymers SAXAMID 226F7 Nylon 6.6, 35% Glass Fiber
SAXAMID 226F7 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 35% glass fibers. It has very high mechanical strength in combination with good impact resistance. It is char..
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
|
Polyram PlusTek PA303G6 Nylon 6.6, Heat Stabilized, 30% Glass Fiber
30% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
|
Polyram PlusTek PB302G8 Nylon 6, 40%Glass Fiber
40%glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ASTM-D790 |
|
Polyram Polytron A30B02 Nylon 66, 30% Long Fiber
30% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ASTM-D790 |
|
Polyram Polytron A30N02 Nylon 66, 30% Long Fiber
30% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
|
Polyram PlusTek RA303G6 Nylon 6.6, 30% Glass Fiber
30% glass fiber reinforced, heat stabilized, and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Strength | 290 MPa | 42100 psi | 2 mm/min; ISO 178 |
|
Eurostar Staramide BG8 PA6, 40% Glass Fiber Filled, Injection Molded
Staramide BG8 is a 40% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Flexural Strength | 290 MPa | 42100 psi | 2 mm/min; ISO 178 |
|
Eurostar Staramide AG7 PA66, 35% Glass Filled, Injection Molded
AG7 is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
|
Adell AR-38 Nylon 66, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties ..
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
|
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM
Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free..
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R533T Nylon 66, Translucent, 33% Glass Filled, Dry as Molded
Vydyne® R533T is a translucent 33% glass-reinforced PA66 resin designed specifically for use in power-steeing reservoirs dn other applications where chemical resistance, whiteness and transmittance..
|
|||
| Flexural Strength | 290 MPa | 42100 psi | Dry; ASTM D790 |
|
Asahi Kasei Leona® 14G25 25% Glass Filled Nylon 66
Enhanced strength and stiffness; with 25% GF. Superior heat aging resistance, fatigue resistance, and creep resistance.Applications:Mechanical and electrical parts, engine mounts and other under-the..
|
|||
| Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
|
Asahi Kasei Thermylon® NSG-240A 50% Ceramic and Glass Fiber Reinforced
Information provided by Asahi Thermofil
|
|||
| Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||
| Flexural Strength | 290 MPa | 42100 psi | 5 mm/min; ISO 178 |
|
Gromax CFG45-RN13N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||