Mechanical Properties Metric English Comments
Flexural Strength <= 200 MPa
<= 29000 psi
ISO 178
Polykemi AB SCANAMID 66 A12^ F20 FR6 Nylon 66, Glass Fiber Reinforced, Flame Retardant
Information provided by Polykemi AB
Flexural Strength <= 200 MPa
<= 29000 psi
Polykemi AB SCANMID 6 B12^ F20 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
Flexural Strength 200 MPa
29000 psi
10mm/min; DIN 53452
Qualchem Danamid FGFH-30 Polyamide 6, 30% Glass Fiber
Reinforced with glass fiber. Heat stabilized, for long-lasting use at 120-140°C.Information provided by Qualchem Zrt.
Flexural Strength 200 MPa
29000 psi
at 5% strain; ASTM D790
Shell Carilon® DP R1130 Polyketone, 30% Glass Fiber Reinforced &nbsp;(discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1130 is a 30 percent glass fiber reinforced compound based on a developmental e..
Flexural Strength 200 MPa
29000 psi
Lehmann & Voss LUVOCOM® 1105-8422 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
Flexural Strength 200 MPa
29000 psi
Lehmann & Voss LUVOCOM® 3-7088-1 Polyamide 6, with carbon fiber and glass fiber, low-warpage
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
Flexural Strength 200 MPa
29000 psi
Lehmann & Voss LUVOCOM® 1105-7373 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Chemical and hydrolysis resistan..
Flexural Strength 200 MPa
29000 psi
ASTM D-790
Glastic T-160 Fiberglass-Reinforced Polyester Laminate
Grade T-160 is a new, high-strength, heat-resistant laminate. This highly creep-resistant material is excellent for applications where electrically insulating materials are subject to physical load..
Flexural Strength 200 MPa
29000 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OX88533 PPS
LNP LUBRICOMP* OX88533 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Flexural Strength 200 MPa
29000 psi
SPS Guang Zhou PONYLâ„¢ EP4003G25 Non-halogen flame retardance/GF25%-PA66
Characteristic: Good flame retardance, high mechanical properties, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) Ltd.
Flexural Strength 200 MPa
29000 psi
ASTM D790
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedAppearance: RedInformation provi..
Flexural Strength 200 MPa
29000 psi
ASTM D790
Polyram PlusTek PA320G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant
25% glass fiber reinforced, flame retardant and high stiffness polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Flexural Strength 200 MPa
29000 psi
ASTM-D790
Polyram Polytron P50B03 Copolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber
A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED BLACK POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteristi..
Flexural Strength 200 MPa
29000 psi
ISO 178
DuPont Performance Polymers Crastin® SK605 BK851 Polybutylene Terephthalate (PBT) &nbsp;(Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 BK851 is a 30% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..
Flexural Strength 200 MPa
29000 psi
50%RH; ISO 178
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66 &nbsp;(Unverified Data**)
33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Flexural Strength 200 MPa
29000 psi
50%RH; ISO 178
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance..
Flexural Strength 200 MPa
29000 psi
2 mm/min; ISO 178
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded
AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Flexural Strength 200 MPa
29000 psi
ISO 178
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, Conditioned
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
Flexural Strength 200 MPa
29000 psi
ISO 178
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
Flexural Strength 200 MPa
29000 psi
ASTM D790
Beijing Ranger Chem PBT 403 M-G30 Heat Resistant and Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Flexural Strength <= 200 MPa
<= 29000 psi
cond., 3.5% flexure; ISO 178
Azoty Tarnow™ Tarnamid® T-27 GF35 Polyamide 6 - Glass Fiber Reinforced
35% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Flexural Strength 200 MPa
29000 psi
ISO 178
DuPont Performance Polymers Rynite® FR530L BK507 Polyethylene Terephthalate (PET)
Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Flexural Strength 200 MPa
29000 psi
ISO 178
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, Conditioned
Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Flexural Strength 200 MPa
29000 psi
ISO 178
Polyplastics Duracon® GH-25 Acetal Co-polymer (POM), GF 25% reinforced, High strength, High rigidity
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..