| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 248 MPa | 36000 psi | ASTM D790 |
|
PolyOne Nymax™ GF 604 35 HS Natural Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
|
|||
| Flexural Strength | 248 MPa | 36000 psi | Transverse Rupture |
|
Pacific Sintered Materials F-200-P Iron Powdered Metal
Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-10All information provided by Pacific Sintered Metals.
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ASTM D790 |
|
Polymer Resources NY66-G33 Nylon 66, 33% Glass Reinforced
Nylon 66, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ASTM D790 |
|
Polymer Resources NY66-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ASTM D790 |
|
PolyOne Edgetek® PK-30GF/000 Polyetheretherketone (PEEK)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Flexural Strength | 248 MPa | 36000 psi | |
|
Haysite 54500 Polyester SMC, 35% Glass Reinforced
A high strength fiberglass reinforced thermoset polyester compound formulated for injection, compression, or transfer molding. This material exhibits excellent electrical and mechanical properties, ..
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP PFN16 PA 6 (Asia Pacific)
LNP* Lubricomp* PFL-4216 is a compound based on Nylon 6 resin containing Glass Fiber, MOS2. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ASTM D 790 |
|
SABIC Innovative Plastics LNP Lubricomp UCL24S PPA (Asia Pacific)
LNP* Lubricomp* UCL24S is a compound based on Polyphthalamide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Heat Stabilized, Electrically Cond..
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ASTM D790 |
|
Solvay Specialty Polymers Ryton® R-4-240BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat..
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ASTM D 790 |
|
SABIC Innovative Plastics LNP Thermocomp EF008E PEI
LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas..
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS (Asia Pacific)
LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF006I PA 66
LNP* THERMOTUF* RF006I is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: High Impact.
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 (Asia Pacific)
LNP* Thermocomp* RFB66 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass.
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ASTM D790 |
|
Techmer Lehvoss Compounds Luvotech™ J-4/35 NAT PA6/12
(discontinued **)
Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated.
|
|||
| Flexural Strength | 248 MPa | 36000 psi | ASTM D790 |
|
LNP Thermocomp® QF-1006 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
(discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
|
|||