| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength |
250
MPa <br>@Temperature 23.0 °C
|
36300
psi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement
(discontinu
Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ASTM D790 |
|
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
(Unverified Data**)
AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | |
|
Lehmann & Voss LUVOCOM® 20-7324 Polyphthalamide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | |
|
Lehmann & Voss LUVOCOM® 3-8437 Polyamide 6, with glass fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Emergency running property.Suitable for metall inserts.Control..
|
|||
| Flexural Strength | >= 250 MPa | >= 36300 psi | |
|
MarkeTech AN 120 Aluminum Nitride Ceramic Substrate, 98% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Grupo Repol Dinalon® A1S25 G35PV0 35% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 66
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Kuraray Genestarâ„¢ G1301A-M61 Nylon, 30% Glass Filled
30% Glass reinforced and impact modified injection grade.Main Features:Higher elongation and impact strengthHeat resistanceChemical resistanceExample of applications:Quick connector
|
|||
| Flexural Strength | 250 MPa | 36300 psi | 2 mm/min; ISO 178-A |
|
Lanxess Durethan® BKV 130 H3.0 DUS008 000000 Nylon 6, 30% Glass Fiber
PA 6, glass fiber, injection molding, impact modified, heat-aged stabilizedInformation provided by LANXESS.
|
|||
| Flexural Strength | 250 MPa | 36300 psi | |
|
Lehmann & Voss LUVOCOM® 1105/GF/40/BK-1 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | |
|
Lehmann & Voss LUVOCOM® 1105-0706 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | |
|
Lehmann & Voss LUVOCOM® 1-1108 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber
AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ASTM D790 |
|
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Asia Pacific)
LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP EC004XXC PEI
LNP* THERMOCOMP* EC004XXC is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Flexural Strength | 250 MPa | 36300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear (Europe-Africa-Middle East)
LNP* THERMOCOMP* OC006 is a compound based on PPS - Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
SABIC Innovative Plastics LNP VERTON PX91200 PA 6
LNP VERTON* PX91200 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added features of this material include: High Impact, Structural
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry
Information provided by Unitika Ltd.
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ASTM D790 |
|
Polyram PlusTek PA4801G6 Nylon 6.6, 30% Glass Fiber Reinforced, PTFE lubricated
30% glass fiber reinforced, PTFE lubricated polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ASTM C1161 |
|
M Cubed Technologies TSC-15 Titanium-alloyed Reaction Bonded Silicon Carbide
Specialty reaction-bonded SiC for applications requiring high stiffness, high toughness, and also high thermal conductivity--mechanical seals, for example Flow-through complex channels can be forme..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, Conditioned
Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | at max force; ISO 178 |
|
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Dry)
Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas..
|
|||
| Flexural Strength | 250 MPa | 36300 psi | ISO 178 |
|
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T..
|
|||