Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 37700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Strength 260 MPa
37700 psi
ASTM D790
Gharda Chemicals GATONE™ 5630GF Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
Flexural Strength 260 MPa
37700 psi
Lehmann & Voss LUVOCOM® 1105-8161 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
Flexural Strength 260 MPa
37700 psi
Lehmann & Voss LUVOCOM® 21-7976 Polyamide 6/6T, with glass fiber and PTFE, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Flexural Strength 260 MPa
37700 psi
ISO 178-A
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance
Flexural Strength 260 MPa
37700 psi
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15 Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Flexural Strength 260 MPa
37700 psi
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
Flexural Strength 260 MPa
37700 psi
Lehmann & Voss LUVOCOM® 1105/GF/30/BK-1 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Flexural Strength 260 MPa
37700 psi
5 mm/min; ISO 178
Gromax CFG35-R113N1 Nylon 6 36% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Flexural Strength 260 MPa
37700 psi
Lehmann & Voss LUVOCOM® 1105/GF/40 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
Flexural Strength 260 MPa
37700 psi
ASTM D790
Solvay TECHNYL® A 218 V25 NAT BA PA66, 25% glass fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: Asia PacificProduct Application..
Flexural Strength 260 MPa
37700 psi
ISO 178
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, DRY
Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ..
Flexural Strength 260 MPa
37700 psi
ISO 178
Solvay Technyl® C216V25 25% Glass Filled Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Flexural Strength 260 MPa
37700 psi
ISO 178
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
Flexural Strength 260 MPa
37700 psi
ISO 178
Unitika B2040G33 PA66, 33% Glass Fiber Reinforced, Dry
Information provided by Unitika Ltd.
Flexural Strength 260 MPa
37700 psi
ISO 178-93
Wellman Wellamid® GF1782-BK1 40% Glass Fiber Reinforced Nylon 6
Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman.
Flexural Strength 260 MPa
37700 psi
ISO 178-93
Wellman Wellamid® GF43-66/6 XE-NBK1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman.
Flexural Strength 260 MPa
37700 psi
dry; ISO 178
DSM EcoPaXX® Q-KG6 PA410-GF30
% Glass Reinforced, Heat Stabilized, for E&E applications
Flexural Strength 260 MPa
37700 psi
dry; ISO 178
DSM Novamid® 1013G30 1 NA PA6-GF30
30% Glass Reinforced, Injection Molding
Flexural Strength 260 MPa
37700 psi
dry; ISO 178
DSM Novamid® 3010GN30 NAT PA66-GF30 FR(17)
30% Glass Reinforced, Flame Retardant
Flexural Strength 260 MPa
37700 psi
2 mm/min; ISO 178
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded
AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Flexural Strength 260 MPa
37700 psi
2 mm/min; ISO 178
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded
AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Flexural Strength <= 260 MPa
<= 37700 psi
dry, 3.5% flexure; ISO 178
Azoty Tarnow™ Tarnamid® T-27 GF30 Polyamide 6 - Glass Fiber Reinforced
30% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Flexural Strength 260 MPa
37700 psi
ISO 178
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry)
Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el..
Flexural Strength 260 MPa
37700 psi
ASTM Test
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry)
Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushion ..
Flexural Strength 260 MPa
37700 psi
ISO 178
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Dry)
Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF
Flexural Strength 260 MPa
37700 psi
ASTM D790
Owens Corning Glass Fiber Reinforced Polyphenylene Sulfide, 40 wt.% glass
Polyphenylene Sulfide provides excellent resistance to organic solvents (below 375°F). It is unaffected by strong alkalis or aqueous organic salt solutions. Data provided by the manufacturer, Owen..
Copyright © lookpolymers.com All Rights Reserved