| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 270 MPa | 39200 psi | STN EN ISO 178 |
|
Plastcom SLOVAMID 66 GF 35 Polyamide 66, 35% Glass Fiber
FeaturesChemically reinforced with 35% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | |
|
Plastcom SLOVASTER® E GF 30 PBT, 30% glass fibre
FeaturesPET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Nilit FRIANYL A63 GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Strength | <= 270 MPa | <= 39200 psi | ISO 178 |
|
Polykemi AB SCANAMID 66 A12^ F35 NH9 Nylon 66, Glass Fiber Reinforced, Flame Retardant, Halogen Free
Information provided by Polykemi AB
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
DSM Akulon® K-FG6 (Dry) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | |
|
MarkeTech Zirconium Oxide Ceramic - Zirconia, Y2O3 Stabilized
Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is ..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | |
|
Lehmann & Voss LUVOCOM® 1/GF/40/TF/13 Polyamide 66, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | |
|
Lehmann & Voss LUVOCOM® 1-0889-2 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | 5 mm/min; ISO 178 |
|
Gromax BFG30-FH00B1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL16 PA 66 (Asia Pacific)
LNP LUBRICOMP* RFL16 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber
Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low ..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178-93 |
|
Wellman Wellamid® GF33A099-HRN Nylon 66, 33% Glass Reinforced, Hydrolysis Resistant
All information provided by Wellman Engineered Resins.
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, Conditioned
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry)
Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry)
Information provided by BASF
|
|||
| Flexural Strength | 270 MPa | 39200 psi | 2 [mm/min]; ISO 178 |
|
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded
Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ASTM D790 |
|
Solvay TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY
Description: Polyamid 66, 30% glass fiber reinforce, for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2411GF6 used in all sectors of industry, offering an excellent com..
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
Kuraray Genestar™ G1300A-M41 Nylon, 30% Glass Filled
Glass reinforced injection grade. Main Features:Chemical resistanceHeat resistanceExamples of applications:Gears and bearing retainersIntercooler tank and turbo duct pipe
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ASTM D790 |
|
Kuraray Genestar™ GN2450 Nylon, 45% Glass Filled
High Strength V-0 Grade. Features a high strength and modulus. It is well suited for FPC sliders and IC sockets, as well as other components that require modulus and dimensional precision.
|
|||
| Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
|
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade.
|
|||