Polymer Property : Flexural Strength = 40.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
NYCOA 2084 HS Super-Tough, High Viscosity Nylon 6 Resin
NYCOA 2084 HS is a high viscosity resin particularly suitable for extrusion processing. Its melt viscosity and strength provide ease of processing for tubing, profile, and molded articles. This mate..
Flexural Strength 40.0 MPa
5800 psi
Plastcom SLOVALEN PH 59 GB 20 PP, 20% glass beads, mod. of mech. prop.
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
Flexural Strength 40.0 MPa
5800 psi
ISO 178
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab..
Flexural Strength 40.0 - 50.0 MPa
5800 - 7250 psi
ASTM D790-03
Proto3000 Objet Digital Materials™ DM_4310 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Flexural Strength 40.0 - 50.0 MPa
5800 - 7250 psi
ASTM D790-03
Proto3000 Objet Digital Materials™ DM_4710 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Flexural Strength 40.0 MPa
5800 psi
2 mm/min; ASTM D 790
Polimeri Europa Sinkral® D 232/M3 ABS Resin  (discontinued **)
Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr..
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
Fiberfil® M-2450 Polypropylene Copolymer
Information provided by FIBERFIL Engineered Plastics
Flexural Strength 40.0 MPa
5800 psi
2mm/min; ASTM D790
Kingfa FRHIPS-1162 Flame Retardant Polystyrene
Features:UL 94 V-2 @ 1.6mm, V-2 @ 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingEl..
Flexural Strength 40.0 MPa
5800 psi
ASTM D790 A
Metabolix Mirelâ„¢ P1003 Injection Molding Grade PHA Bioplastic
Mirelâ„¢ P1003 is a general purpose injection molding material with high modulus.Mirel is suitable for a wide range of injection molded food service and packaging applications including caps and ..
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
Lucent Polymers CPP-310 Polypropylene, 10% Calcium Carbonate Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Strength 40.0 MPa
5800 psi
2mm/min; ASTM D790
Kingfa FRHIPS-8002 Flame Retardant Polystyrene
Features:UL 94 V-2 @ 1.0mm, V-2 @ 3.2mmExcellent balancing properties, Non-DPOExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElec..
Flexural Strength 40.0 MPa
5800 psi
conditioned, 2 mm/min; ISO 178-A
Lanxess Durethan® AC 30 DUS027 000000 Nylon 66
PA 66, non-reinforced, injection molded, impact modifiedInformation provided by LANXESS.
Flexural Strength 40.0 MPa
5800 psi
ISO 178
Solvay TECHNYL® PSB 286 PA6, Conditioned
Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.Available in: North AmericaProduct Applications: This grade has high fl..
Flexural Strength 40.0 MPa
5800 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON CD000I PS
LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Flexural Strength 40.0 MPa
5800 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON MX01739C PP
LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
Flexural Strength 40.0 MPa
5800 psi
SPS Guang Zhou SAMATâ„¢ EP 5001C(f1) Flame-retarded Polypropylene
Characteristic: Good flame retardance, non-halogen, high flow properties, high rigidity, high heat resistance, meets the requirements of RoHs and PaHs, excellent UV resistanceApplications: X'mas dec..
Flexural Strength 40.0 MPa
5800 psi
ISO 178
Styrolution PS 542N HIPS
Styrolution PS 542N is an impact polystyrene with high heat resistance.Information provided by Styrolution
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
A. Schulman POLYFORT™ FXP 2779U UV Stabilized Copolymer Polypropylene
DescriptionPolyfort® FXP 2779U is a 20% talc-filled, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
Flexural Strength 40.0 MPa

@Treatment Temp. 150 °C,
Time 3600 sec
5800 psi

@Treatment Temp. 302 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Sheets
Description: Electrical and electrotechnical applications. Suitable as high-frequency insulation on account of its dielectric loss. Used as, among other things, an insulation material in large induc..
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0334M10L Mica Reinforced
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0336M10L Mica Reinforced
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0339W20L1 Wollastonite Reinforced
Flexural Strength 40.0 MPa
5800 psi
at max force; ISO 178
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Conditioned)
Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector..
Flexural Strength 40.0 MPa
5800 psi
ISO 178
BASF Ultramid® S3K Balance PA 610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0436G10CL Glass Reinforced
Flexural Strength 40.0 MPa
5800 psi
2 mm/min; ISO 178
Polimeri Europa Edistir N 2982 Polystyrene
General purpose polystyrene with very high flow and high heat resistance. Special grade for direct gassing extrusion of heavy gage insulating boards (XPS) foamed by blowing agents alternative to CFC..
Flexural Strength 40.0 MPa
5800 psi
ISO 178
Polyram RamOfin PPC361T4 Polypropylene, 20% Mineral Filled
20% Mineral filled, heat resistant polypropylene for injection molding applications.Information provided by Polyram.
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
A. Schulman POLYFORT™ FXP 2779U UV Stabilized Copolymer Polypropylene
DescriptionPolyfort® FXP 2779U is a 20% talc-filled, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
Flexural Strength 40.0 MPa
5800 psi
2 mm/min; ISO 178
Sax Polymers SAXALEN PPH329B20 Polypropylene Homopolymer, 20% Glass Filled
SAXALEN PPH329B20 is a 20% glass beads filled Polypropylene - Homopolymer intended for injection molding. Low shrinkage, low warpage gradeInformation provided by SAX Polymers