Polymer Property : Flexural Strength = 55.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Strength 55.8 MPa
8090 psi
ASTM D790
PolyOne Maxxam™ PD 40 TF Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Strength 55.8 MPa
8090 psi
Poco Graphite EDM-200 EDM Graphite
POCO's EDM-200 is an isotropic Superfine particle graphite providing good strength, surface finish, and wear resistance.Applications:Structural ribsRoughing or finishing electrodesLarge featured mol..
Flexural Strength 55.8 MPa
8100 psi
Ohio Carbon Blank OCB EDM-200 Mechanical Grade Graphite
Available in a range of sizes and shapes.
Flexural Strength 55.8 MPa
8100 psi
ASTM D790
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified
Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Flexural Strength 55.8 MPa

@Temperature 175 °C
8090 psi

@Temperature 347 °F
4; ISO 178
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Flexural Strength 55.8 MPa
8090 psi
ASTM D790
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp
Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and..
Flexural Strength 55.8 MPa
8100 psi
ASTM D790
Chesterton ARC MXHT High temperature severe wear compound
Description: An advanced ceramic composite for the protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack at elevated temperatures. It is applied at a thickness o..
Flexural Strength 55.8 MPa
8100 psi
3M Scotchkote™ CR 511 Epoxy Ceramic Surface
Scotchkote Epoxy Ceramic CR 511 has been specifically developed as a 100% solids coating for resurfacing and lining to improve the efficiency of equipment in fluid flow environments.Product Features..
Flexural Strength 55.8 MPa
8100 psi
BCC Products BC 7062-2H Epoxy Casting
BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi..
Flexural Strength 55.8 MPa

@Temperature 175 °C
8090 psi

@Temperature 347 °F
ISO 178
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..