| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 60.0 MPa | 8700 psi | STN EN ISO 178 |
|
Plastcom SLOVAMID 66 HI Polyamide 66, Impact Grade
FeaturesModified with thermoplastic reactive elastomer, determined for mouldings with high toughness also at low temperatures. Eligible application for ski-shoes, helmets for sport and other safety..
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
|
Nilit FRIANYL A63 H-SG40 Nylon 6.6 for injection molding, 40% mineral filled
Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
|
Nilit RECONYL B S Recycled nylon 6 for injection molding
Recycled nylon 6 for injection molding, impact modified (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Strength | 60.0 - 70.0 MPa | 8700 - 10200 psi | Compression; ISO 178 |
|
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
|
|||
| Flexural Strength | 60.0 - 80.0 MPa | 8700 - 11600 psi | Injection; ISO 178 |
|
Raschig Group 4554 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi..
|
|||
| Flexural Strength |
60.0
MPa @Temperature 100 °C |
8700
psi @Temperature 212 °F |
ISO 178 |
|
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
(
AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer..
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ASTM D790 |
|
Ineos Nova 1552 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
Easy processing, High modulus, Improve stress whitening, Custom colorsApplications: Injection molding, Office furniture, Electronic media, Photographic equipmentPerformance grades of polystyrene are..
|
|||
| Flexural Strength |
60.0
MPa @Strain 3.50 %, Temperature 23.0 °C |
8700
psi @Strain 3.50 %, Temperature 73.4 °F |
ISO 178 |
|
DuPont Performance Polymers Delrin® 500T BK602 Acetal Homopolymer
(Unverified Data**)
Delrin® 500T BK602 is a toughened, medium viscosity acetal homopolymer resin with impact resistance similar to Delrin® 100. It can be used in parts requiring noise reduction.Information provided b..
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | |
|
Lehmann & Voss LUVOCOM® 6-8436 Polyamide 12, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve..
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | |
|
Lehmann & Voss LUVOCOM® 80-7580/BK Polyacetal-copolymer, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | |
|
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | 2mm/min; ASTM D790 |
|
Kingfa HF-626 Flame Retardant ABS
Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowHigh impact resistanceApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | DIN 54352 |
|
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned
Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
|
Styrolution Luran® S 797 S White 35962 ASA
Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
|
Styrolution Novodur® M210TF ABS
Novodur M210TF is medium impact, high gloss injection molding grade designed for toy application. M210TF is in compliance with food contact regulationsInformation provided by Styrolution
|
|||
| Flexural Strength |
60.0
MPa @Thickness 3.17 mm |
8700
psi @Thickness 0.125 in |
ASTM D790 |
|
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP SH0700B PA12
LNP* Thermocomp* SH0700B is a compound based on Nylon 12 containing proprietary fillers. Added feature: High Specific Gravity
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
|
Tisan TISAPET® 20% Glass Reinforced Polyethylene Terephthalate
Properties:Excellent mechanical propertiesHigh thermal-chemical friction resistanceGood electrical propertiesGood rate of melt flow index relative to the quantity of glass fiberBalanced electrical a..
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178-93 |
|
Wellman Wellamid® XT1668-BK1 High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ASTM-D790 |
|
Polyram RamTal PM8427 Acetal, Impact modified
Impact modified polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | dry; ISO 178 |
|
DSM Novamid® ST120 NAT PA6-I
Impact Modified, Injection Molding
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | 2 mm/min; ISO 178 |
|
Chi Mei Polylac® PA-746 ABS - High Flow
High flow, medium impact
|
|||
| Flexural Strength |
60.0
MPa @Strain 3.50 % |
8700
psi @Strain 3.50 % |
ISO 178 |
|
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
|
Azoty Tarnow™ TARNOFORM 300 SI POM
Tribological modified grade with silicon, for better sliding properties in plastic-plastic contact.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ASTM D790 |
|
Ravago Manufacturing Americas Enviramid™ N2300STHL BK Post Consumer Recycle Nylon 6
Superior Toughness, Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
|
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific)
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa..
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
|
Polyram RamLloy PVB702 Nylon/ABS Alloy, Impact Modified
Impact modified, UV stabilized Nylon/ABS alloy for injection molding applications.Information provided by Polyram.
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
|
Lucite International Diakon® ST45G8 Toughened Acrylic Polymer
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in..
|
|||
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
|
Polyram RamTal PM340S6 Polyacetal for Injection Molding, 30% Glass-Beads Filled
30% Glass-beads filled polyacetal for injection molding applications.Information provided by Polyram.
|
|||