| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and ..
|
|||
| Flexural Strength | <= 79.0 MPa | <= 11500 psi | ISO 178 |
|
Polykemi AB POLYabs X00 ABS, Extrusion Grade
Information provided by Polykemi AB
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | |
|
Lehmann & Voss LUVOCOM® 80-8387 Polyacetal-copolymer, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, ..
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | |
|
Lehmann & Voss LUVOCOM® 80-8470 Polyacetal-copolymer, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, ..
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
Kolon SPESIN® KP513 PBT Alloy Resin
Excellent extrudable and SpinningApplications: Mono filamentInformation provided by API-Kolon.
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
Kolon SPESIN® KP513UG PBT Alloy Resin
Extrudable, delusteringApplications: Mono filamentInformation provided by API-Kolon.
|
|||
| Flexural Strength |
79.0
MPa <br>@Temperature 22.0 °C
|
11500
psi <br>@Temperature 71.6 °F
|
25 mm wide 100 mm long, flat samples; ISO 14125 |
|
Menzolit Menzolit® BMC 3100 Unsaturated Polyester UP
BMC 3100 is a special BMC suitable for the use in head lamp reflectors. Because of its high temperature resistance and dimensional stability as well as low coefficient of thermal expansion, complex ..
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
LG Chemical LUPOY GN-5001TF Halogen Free PC/ABS Alloy, High Flow, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU
LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU (Asia Pacific)
LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer
LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized.
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer (Asia Pacific)
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East)
XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I.
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR
LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D 790 |
|
SABIC Innovative Plastics LNP Thermocomp YF006 TPEE
LNP THERMOCOMP* YF006 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ISO 178 |
|
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA (Asia Pacific)
LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pacific ..
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
SABIC Innovative Plastics NORYL N190HF PPE+HIPS (Asia Pacific) |
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF)
LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive.
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Asia Pacific)
PPE/PS, 80degC, FR V-0, high flow
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
Plenco 3356 Phenolic, Granular, Injection Molded
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i..
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
Plenco 4527 Phenolic, Granular, Injection Molded
PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under..
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
Plenco 7591 Phenolic, Briquette, Injection Molded
PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (Conditioned)
Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo.
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
Plenco 4301 Phenolic, Granular, Injection Molded
PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava..
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
Plenco 4504 Phenolic, Granular, Injection Molded
Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c..
|
|||
| Flexural Strength | 79.0 - 121 MPa | 11500 - 17500 psi | ASTM D790M |
|
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure
DescriptionNanoTool produces strong, stiff, high temperature resistant composite parts on conventional stereolithography machines. This third generation of Somos® ProtoComposite materials is heavi..
|
|||
| Flexural Strength |
79.0
MPa <br>@Strain 3.50 %
|
11500
psi <br>@Strain 3.50 %
|
ISO 178 |
|
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | 23°C, 50% RH; ASTM D790 |
|
Asahi Kasei Xyron® 340W Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
|
|||
| Flexural Strength | 79.0 MPa | 11500 psi | ASTM D790 |
|
Ashley Polymers Ashlene® PC/ABS Alloy
Flame retardant alloy.Data provided by the manufacturer
|
|||