| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Multibase Nylex™ 2112 FR V0 Natural Polyamide + PP
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Polymer Resources PPX-FR1-[color]EN Modified PPO, UL 94 V-0 with HDT of 190 F, Extrusion Grade
Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont
Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
PolyOne Lubri-Tech™ ATH-5KV/000 Acetal-Homopolymer, Aramid Fiber
(discontinued **)
Description/Features:Aramid Fiber ReinforcedInformation provided by PolyOne Corporation.
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
MRC Polymers SATRANâ„¢ 800R ABS Terpolymer, Reprocessed
black onlyInformation provided by MRC Polymers Inc.
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | |
|
SGL Carbon Group EK 20 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Techmer ES Electrablend® POM C BK Acetal
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive and CopolymerAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Techmer ES HiFill FR® PA6 FR IM
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc.
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Techmer ES HiFill® HDPE GF15 BK 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Flexural Strength |
55.2
MPa <br>@Thickness 3.17 mm
|
8000
psi <br>@Thickness 0.125 in
|
ASTM D790 |
|
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS
VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Strength |
55.2
MPa <br>@Thickness 3.17 mm
|
8000
psi <br>@Thickness 0.125 in
|
ASTM D790 |
|
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS
VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Teknor Apex Chemlon® 267 Nylon 6, Impact Modified
Notes: Chemlon® is a product offering flexural modulus, impact and elongation properties suitable for convoluted tubing and wire coating applications. Features: Copolymer; Good Flexibility; Good ..
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Techmer ES HiFill FR® PA6 E FR
Availability: North AmericaForms: PelletsFeatures: Flame Retardant Processing Method: ExtrusionInformation provided by TP Composites, Inc.
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Chase Plastics CP Pryme® NN100STL (DAM) Nylon 66, Super Toughened, Internally Lubricated
Information provided by Chase Plastics.
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static)
Non-carbon filled anti-static material which has high impact strength, good tensile and flexural strength, and is easily machined. Available in natural or black, it can be easily thermoformed in th..
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Ecomass® 4703ZD84 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technica..
|
|||
| Flexural Strength | <= 55.2 MPa | <= 8000 psi | ASTM D790 |
|
Arkema Group Solarkote® PB Acrylic
For PVC/acrylic alloys Information provided by Arkema Group
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Americas Styrenics MC3650 High Heat Crystal Polystyrene
Product CharacteristicsImproved cycle times in hard to fill partsExcellent clarity with slight blue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsHousewaresConsumer..
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Aremco Aremco-Bond™ 820 High Performance Epoxide
Clear, 1:1, 45-Minute Cure System with Good Flexibility
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
|
PolyOne Edgetek® UR-30GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||