Polymer Property : Flexural Strength = 87.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Strength <= 87.0 MPa
<= 12600 psi
ISO 178
Polykemi AB POLYasa 2410F High Flow ASA
Information provided by Polykemi AB
Flexural Strength 87.0 - 125 MPa
12600 - 18100 psi
ASTM D790
Proto3000 Accura® Amethyst™ Material for use with Viper™ SLA® systems
Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. FEATURES:Outstanding accuracyExceptional detailHigh thermal resistanceDeep purple colorLow as..
Flexural Strength 87.0 MPa
12600 psi
ISO 178
Nilit FRIANYL A63 HS-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced
Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Flexural Strength 87.0 MPa
12600 psi
ISO 178
PTS POM-90 Acetal Copolymer
Information provided by PTS LLC.
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DL002F PC
LNP LUBRICOMP* DL002F is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Superior Molding.
Flexural Strength 87.0 MPa
12600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN
LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati..
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
Kolon KOCETAL® LW701 Wear Modified Acetal Resin
Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon.
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY D20009 PC
LNP LUBRILOY* D20009 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Flame Retardant, Wear Resistant.
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX93500 PC
LNP STAT-KON* DX93500 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Flexural Strength 87.0 MPa
12600 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP MF741XXH PP
LNP* THERMOCOMP* MF741XXH is a compound based on Polypropylene reain containing Glass Fiber and proprietay antimicrobial additives. Designed for touch surfaces in patient critical healthcare applic..
Flexural Strength 87.0 MPa
12600 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched
LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region.
Flexural Strength 87.0 MPa
12600 psi
ISO 178
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR
LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region.
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
SABIC Innovative Plastics NORYL PX1340 PPE+HIPS (Asia Pacific)
PPE+PS MF Filled
Flexural Strength 87.0 MPa
12600 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP MF742XXH PP
LNP* THERMOCOMP* MF742XXH is a compound based on Polypropylene resin containing Glass Fiber and proprietary antimicrobial additives. This product is best suited for touch surfaces in healthcare app..
Flexural Strength 87.0 MPa
12600 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RB006 PA 66
LNP* THERMOCOMP* RB006 is a compound based on Nylon 66 resin containing 30% Glass Bead.
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
Plenco 6343 Phenolic, Granular, Transfer Molded
PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz..
Flexural Strength 87.0 MPa
12600 psi
ISO 178
Polyplastics Tepcon M90 Acetal-copolymer (POM), General
Information provided by PolyPlastics.
Flexural Strength 87.0 MPa
<br>@Strain 3.50 %
12600 psi
<br>@Strain 3.50 %
ISO 178
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM) &nbsp;(Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s..
Flexural Strength 87.0 MPa
<br>@Strain 3.50 %
12600 psi
<br>@Strain 3.50 %
ISO 178
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM) &nbsp;(Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..
Flexural Strength 87.0 MPa
12600 psi
ASTM Test
BASF Ultramid® 8253 PA6 (Dry)
Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o..
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
A. Schulman ComAlloy Aqualoy® 125 Polypropylene, Glass Reinforced, Chemically Coupled NSF, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an..
Flexural Strength 87.0 - 101 MPa
12600 - 14600 psi
ASTM D790
3D Systems Accura® 60 Plastic for SLA® Systems
Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr..
Flexural Strength 87.0 - 125 MPa
12600 - 18100 psi
ASTM D790
3D Systems Accura® Amethyst™ Plastic for Viper™ SLA® Systems
Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. For use with Viper™ SLA® systems.ApplicationsPatterns for use with low and high vulcanizing..
Flexural Strength 87.0 MPa
12600 psi
ISO 178
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity..
Flexural Strength 87.0 MPa
12600 psi
ISO 178
Polyplastics Duracon® CP-15X Acetal Co-polymer (POM), Creep resistant, Creep resistant
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Flexural Strength 87.0 MPa
12600 psi
ISO 178
Polyplastics Duracon® M90-45 Acetal Co-polymer (POM), Weather resistance, General
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Flexural Strength 87.0 MPa
12600 psi
ISO 178
Polyplastics Duracon® M90-71 Acetal Co-polymer (POM), Heat resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Flexural Strength 87.0 - 101 MPa
12600 - 14600 psi
ASTM D790
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer
Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView ..
Flexural Strength 87.0 MPa
12600 psi
ISO 178
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..