| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Oxford Polymers PC 912 Unfilled Polycarbonate for Injection and Extrusion Molding
Unfilled Polycarbonate for Injection and Extrusion MoldingInformation provided by Oxford Polymers.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced
Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigm..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Polymer Resources PC-GP1-[color]-LF Polycarbonate, General Purpose, Food Contact
Polycarbonate, General Purpose, Low FlowFeatures: • Food Contact AcceptableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, ..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release
Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | 1.3 mm/min; ASTM D790 |
|
PolyOne Edgetek® AT-15CF/000 BLACK Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced
Acrylonitrile Butadiene Styrene, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
|
|||
| Flexural Strength |
96.5
MPa @Thickness 3.17 mm, Temperature 22.8 °C |
14000
psi @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D790 |
|
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release
Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package ..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Techmer ES HiFill® PA6/6 GF8 IM4 HS L 8% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 8% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Compo..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Techmer ES HiFill® PET GF15 X BK 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Techmer ES Luriblend® PA6/12 01430 Nylon 612
Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided by TP Composites, Inc.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | Method I (3 point load), 2.0 mm/min; ASTM D790 |
|
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Styron CALIBREâ„¢ 301-10 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Styron CALIBREâ„¢ 303V-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300V-10 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are avai..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | 0.125 in, injection molded, unannealed; ASTM D790 |
|
Styron EMERGEâ„¢ 4330-22 Polycarbonate
EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Styron CALIBREâ„¢ 301 EP Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | Method I (3 point load), 2.0 mm/min; ASTM D790 |
|
Styron CALIBREâ„¢ MEGARAD 2081-HD-15 2 Polycarbonate Resin
Overview: CALIBREâ„¢ MEGARAD 2081 HD-15 2 polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed ..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D638 |
|
Plastics Group Polifil® GFRMPPCC-40 40% Glass Reinforced Polypropylene, High Impact
Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Chase Plastics CP Pryme® NN100HL (Dry) Nylon 66, Heat Stabilized, Lubricated
Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Entec Hylex® P1017FR Polycarbonate
Information provided by Ravago.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Asahi Kasei Thermylene® P6-20FG-2153R 20% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Asahi Kasei Thermylene® P6-30FG-0708 30% Glass Fiber Reinforced, High Impact
Information provided by Asahi Thermofil
|
|||
| Flexural Strength | 96.5 - 138 MPa | 14000 - 20000 psi | |
|
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade
BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings.
|
|||