| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Yield Strength |
0.00172
-
0.00931
MPa @Strain 25.0 % |
0.250
-
1.35
psi @Strain 25.0 % |
0.2"/min. strain rate |
|
Rogers Corporation Poron® 4790-92-09 Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
|
|||
| Compressive Yield Strength |
0.00172
-
0.0172
MPa @Strain 25.0 % |
0.250
-
2.50
psi @Strain 25.0 % |
0.2"/min. strain rate |
|
Rogers Corporation Poron® 4790-92-12 P Series Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
|
|||
| Compressive Yield Strength | 0.00172 - 48.0 MPa | 0.250 - 6960 psi | Average value: 2.16 MPa Grade Count:134 |
|
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..
|
|||