Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.210 MPa
30.5 psi
Ultracor® UKF-85-1/4-1.5 Honeycomb Core Material
Construction: ±45° K49 108. Fiber: Kevlar® K49. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures.  It is expected that it will be..
Compressive Yield Strength 0.210 MPa
30.5 psi
Parallel to thickness @ 10% compression
Zircar Zirconia ZYC Zirconia Cylinders Insulation
Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing ..
Compressive Yield Strength 0.210 MPa
30.5 psi
Static, 70% Compression, ASTM D1621
Covestro Bayfill® EA 4001 Polyurethane Energy-Absorbing Semi-Rigid Foam, Rigid Grade, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Compressive Yield Strength 0.210 MPa
30.5 psi
Compressive Load Deflection at 10%; ASTM D575
Aearo E-A-R Specialty Composites VersaDamp™ V-2325 TPE
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded..
Compressive Yield Strength 0.210 MPa
30.5 psi
Parallel to thickness @ 10% compression
Zircar Zirconia ZYC Zirconia Cylinders Insulation
Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing ..