| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Yield Strength | 206 MPa | 29900 psi | ASTM D695 |
|
Plenco 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound
(discontinued **)
Plaslok 506 is a two-stage, mineral-filled phenolic molding compound. It is formulated for automotive ashtrays and for appliance applications such as utensil handles receiving repeated exposure to ..
|
|||
| Compressive Yield Strength | 206 MPa | 29900 psi | ASTM D695 |
|
Plenco 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **)
Plaslok 5303 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in appliance, automotive and electrical applications. It can be molded by compression, transfer or i..
|
|||
| Compressive Yield Strength | 206 MPa | 29900 psi | ASTM D695 |
|
Plaslok 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 506 is a two-stage, mineral-filled ph..
|
|||
| Compressive Yield Strength | 206 MPa | 29900 psi | ASTM D695 |
|
Plaslok 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5303 is a two-stage, mineral and floc..
|
|||