| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Modulus | 2.76 GPa | 400 ksi | |
|
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded |
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Quadrant EPP Ertalyte® TX Internally Lubricated Semi-Crystalline Polyester (ASTM Product Data Sheet) |
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Quadrant EPP Nylatron® GSM Nylon, Cast MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near ..
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet) |
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | TM R050-38 |
|
Resinlab® EP1385 Black Epoxy Formulation
Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w..
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | TM R050-38 |
|
Resinlab® EP1385 Clear Epoxy Formulation
Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w..
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | TM R050-38 |
|
Resinlab® EP1390 Medium Viscosity, Self Extinguishing Flame Retardant Epoxy Casting Resin System
Resinlab™ EP1390 is a RoHS compliant, medium viscosity, self extinguishing flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Labor..
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Quadrant EPP Semitron® CMP LL5 Polyester (ASTM Product Data Sheet)
Enhanced semi-crystalline polyester product for extended service in CMP retaining rings. Superior performance, especially in oxide processes, and cost effective relative to standard ring materials. ..
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet) |
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Quantum Acetal-Copolymer
Information provided by Quantum Advanced Engineering Plastics
|
|||
| Compressive Modulus | 2.76 - 5.58 GPa | 400 - 809 ksi | Average value: 4.34 GPa Grade Count:4 |
|
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E..
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Spartech Polycast MP 1.25 (UL 752 Level 1) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Spartech Polycast SAR HP 1.25 (UL 752 Level 3) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Spartech Polycast SP 1.25 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | |
|
Engineered Syntactic Systems AZ-40 Deep Water Syntactic Foam
Syntactic foams are a combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high c..
|
|||
| Compressive Modulus |
2.76
GPa @Temperature 22.8 °C |
400
ksi @Temperature 73.0 °F |
ASTM D695 |
|
Quadrant EPP Duratron® U2100 OEI Extruded 10% Glass Reinforced Polyetherimide |
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
|
Quadrant EPP Nylatron® MC® 907 Natural Nylon, Monocast® FDA Compliant, Unfilled Type 6 (ASTM Product Data Sheet) |
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | |
|
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | TM R050-38 |
|
Resinlab® EP1199 Black Unfilled Epoxy Adhesive
Resinlab™ EP1199 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and..
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | TM R050-38 |
|
Resinlab® EP11HT Gray Filled Epoxy Adhesive
Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..
|
|||
| Compressive Modulus | 2.76 GPa | 400 ksi | TM R050-38 |
|
Resinlab® EP1199 Clear Unfilled Epoxy Adhesive
Resinlab™ EP1199 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and..
|
|||