| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | 230 MPa | 33400 psi | d.a.m.; ISO 2039-1 |
|
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced
PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS.
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | ISO 2039-1 |
|
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers
PA 66, 30% glass fibers, injection molding, heat-ageing stabilized
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | dry; ISO 2039-1 |
|
EMS-Grivory Grivory® AG-30 H PA66
Product description: Grilon AG-30 H black 9836 is a normal viscosity, specially heat stabilized PA 66 injection molding grade with 30% glass fibres. Grilon AG-30 H black 9836 has the following impor..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | dry; ISO 2039-1 |
|
EMS-Grivory Grivory® AG-30 PA66-GF30
Information provided by EMS Grivory
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | dry; ISO 2039-1 |
|
EMS-Grivory Grivory® BG-30 FC PA6-GF30
Product description: Grilon BG-30 FC is a heat stabilised PA6 injection moulding grade with 30% glass fibres. Grilon BG-30 FC has the following important properties: High stiffnessExcellent surface ..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | conditioned; ISO 2039-1 |
|
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40
Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | conditioned; ISO 2039-1 |
|
EMS-Grivory Grivory® GV-4 FWA nat PA*-GF40
Product description: Grivory GV-4 FWA natural is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | conditioned; ISO 2039-1 |
|
EMS-Grivory Grivory® GVL-4H nat PA*-GF40
Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | conditioned; ISO 2039-1 |
|
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30
Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | conditioned; ISO 2039-1 |
|
EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30
Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | conditioned; ISO 2039-1 |
|
EMS-Grivory Grivory® TSGL-60/4 black 9839 PA666-GF60
Product description: Grilon TSGL-60/4 black 9839 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black 9839 is characterized by the foll..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | conditioned; ISO 2039-1 |
|
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60
Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following ..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | conditioned; ISO 2039-1 |
|
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40
Product description: Grivory XE 4101 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | dry; ISO 2039-1 |
|
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55
Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | dry; ISO 2039-1 |
|
EMS-Grivory Grivory® XE 4116 nat PA1010-GF55
Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted ..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | conditioned; ISO 2039-1 |
|
EMS-Grivory Grivory® GV-4H PA*-GF40
Product description: Grivory GV-4H natural is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide...
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | conditioned; ISO 2039-1 |
|
EMS-Grivory Grivory® LBV-65H FWA black 9225 PA12-GF65
Product description: Grilamid LBV-65H FWA black 9225 is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features High stiffness combined..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | conditioned; ISO 2039-1 |
|
EMS-Grivory Grivory® LBV-65H FWA nat PA12-GF65
Product description: Grilamid LBV-65H FWA natural is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
|
|||
| Ball Indentation Hardness |
230
MPa <br>@Load 36.5 kg
|
33400
psi <br>@Load 80.5 lb
|
dry; ISO 2039-1 |
|
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced
50% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | value at 30 sec.; ISO 2039-1 |
|
CENTROPLAST CENTROPEEK Polyetheretherketone
This plastic has high temperature resistance, good chemical resistance, and good mechanical characteristics. Its has good sliding friction properties and is suitable for use with foodstuffs or medi..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | H961/30; ISO 2039-1 |
|
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | HB 961/30; ISO 2039-1 |
|
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Dry, 30% Glass Filled
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | HB 961/30; ISO 2039-1 |
|
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | H 961/30; ISO 2039-1 |
|
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||
| Ball Indentation Hardness | 230 MPa | 33400 psi | conditioned; ISO 2039-1 |
|
EMS-Grivory Grivory® GV-4H black PA*-GF40
Product description: Grivory GV-4H black 9915 is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
|
|||