Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.220 - 0.880 J/cm²
<br>@Temperature -30.0 - -30.0 °C
1.05 - 4.19 ft-lb/in²
<br>@Temperature -22.0 - -22.0 °F
Average value: 0.539 J/cm² Grade Count:7
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Charpy Impact, Notched 0.220 J/cm²
<br>@Temperature 23.0 °C
1.05 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage &nbsp;(dis
Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l..
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ASTM D256
Plenco 7300 Phenolic, Nodular, Transfer Molded &nbsp;(discontinued **)
Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file..
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ASTM D256
Plenco 7466 Phenolic, Granular, Transfer Molded &nbsp;(discontinued **)
Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E406..
Charpy Impact, Notched 0.220 J/cm²
<br>@Temperature 23.0 °C
1.05 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179-1/1eA
FKuR Kunststoff Terralene® WF 3516 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® CMH454 Acrylic Polymer
Information provided by Lucite International
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® CMH454L Acrylic Polymer
Information provided by Lucite International
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® MH254 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..
Charpy Impact, Notched 0.220 J/cm²
<br>@Temperature 23.0 °C
1.05 ft-lb/in²
<br>@Temperature 73.4 °F
80x10x4mm, r=0.25; V-notch; ISO 179/1eA
SYNTHOS Krasten® FB28 High Impact Polystyrene And Polyethylene Blend
Polymer blend HIPS/PE. High toughness, very good tensile properties and environmental stress cracking resistance. Processed mainly by extrusion and thermoforming. Production of sheets and films, tec..
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ASTM D256
Plenco 3509 Phenolic, Granular, Compression Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ASTM D256
Plenco 4466 Phenolic, Granular, Transfer Molded
PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466..
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ASTM D256
Plenco 7507 Phenolic, Granular, Transfer Molded
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut..
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ASTM D256
Plenco 6554 Phenolic, Granular, Compression Molded &nbsp;(discontinued **)
Two-Stage Phenolic. PLENCO 06554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 06554 is available in black.Information supp..
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® A 31T1 MZ40 PA66, 40% mineral fiber, DRY
Description: Flame retardant polyamide PA66, 40% mineral filled, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This..
Copyright © lookpolymers.com All Rights Reserved