| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
0.250
-
0.350
J/cm² <br>@Temperature 23.0 °C
|
1.19
-
1.67
ft-lb/in² <br>@Temperature 73.4 °F
|
Injection and Compression; ISO 179/ 1eA |
|
Raschig Group 3535 Epoxy
Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack..
|
|||
| Charpy Impact, Notched | 0.250 - 0.450 J/cm² | 1.19 - 2.14 ft-lb/in² | Compression; ISO 179/1eA |
|
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
|
|||
| Charpy Impact, Notched | 0.250 - 0.350 J/cm² | 1.19 - 1.67 ft-lb/in² | Compression; ISO 179/1eA |
|
Raschig Group RALUPOL® 4802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
|
|||
| Charpy Impact, Notched | 0.250 - 0.350 J/cm² | 1.19 - 1.67 ft-lb/in² | Compression; ISO 179/1eA |
|
Raschig Group RALUPOL® 5000 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all..
|
|||
| Charpy Impact, Notched |
0.250
-
2.50
J/cm² <br>@Temperature -30.0 - -20.0 °C
|
1.19
-
11.9
ft-lb/in² <br>@Temperature -22.0 - -4.00 °F
|
Average value: 0.841 J/cm² Grade Count:49 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
|
|||
| Charpy Impact, Notched | 0.250 - 0.500 J/cm² | 1.19 - 2.38 ft-lb/in² | Average value: 0.360 J/cm² Grade Count:6 |
|
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va..
|
|||
| Charpy Impact, Notched | 0.250 - 0.350 J/cm² | 1.19 - 1.67 ft-lb/in² | Compression; ISO 179/1eA |
|
Raschig Group RALUPOL® 802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up..
|
|||
| Charpy Impact, Notched |
0.250
-
1.24
J/cm² <br>@Temperature -30.0 - -30.0 °C
|
1.19
-
5.90
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 0.640 J/cm² Grade Count:24 |
|
Overview of materials for Nylon 12, Extrusion/Tubing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values ..
|
|||
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179 |
|
Manifattura Cattaneo PET+PTFE Polyethylene Terephthalate
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
|
|||
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179-2:1999 |
|
Global EPP PET SL PET + Solid Lubricant
PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani..
|
|||
| Charpy Impact, Notched |
0.250
J/cm² <br>@Temperature -23.0 °C
|
1.19
ft-lb/in² <br>@Temperature -9.40 °F
|
DIN 53453 |
|
Global PP-1100-PK Polypropylene Homopolymer
Description-transparency, high stiffness, high heat resistantApplications-general purpose, household goodsInformation provided by Global Polymers Corporation.
|
|||
| Charpy Impact, Notched |
0.250
J/cm² <br>@Temperature -23.0 °C
|
1.19
ft-lb/in² <br>@Temperature -9.40 °F
|
DIN 53453 |
|
Global PP-1111-R Polypropylene Homopolymer
Description-transparency, high stiffness, high heat resistantApplications-electrical/electronic Information provided by Global Polymers Corporation.
|
|||
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | |
|
LATI Latiohm 75/4-10 CNT PBT
Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
|
|||
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | |
|
LATI Latiohm 82-02 PD09 PA12
Semiconductive/dissipative product based on Polyamide 12 (PA12). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr..
|
|||
| Charpy Impact, Notched |
0.250
J/cm² <br>@Temperature 23.0 °C
|
1.19
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Styrolution Luran® 388 S SAN
Description: Specialty grade with highest mechanical strength and chemical resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Charpy Impact, Notched |
0.250
J/cm² <br>@Temperature -20.0 °C
|
1.19
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179/1eA |
|
Borealis Daplen™ MD206U Polypropylene Compound 20% Mineral Filled
Daplen MD206U is a 20% mineral filled polypropylene compound intended for injection molding. MD206U has been developed especially for automotive interior parts that require excellent balance betwee..
|
|||
| Charpy Impact, Notched |
0.250
J/cm² <br>@Temperature 23.0 °C
|
1.19
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Unipetrol PP MONSTEN® MA 230 Polypropylene Homopolymer
Applications include injection molding. Antistatic stabilization. Homopolymer.Information provided by Unipetrol RPA
|
|||
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179/1eA |
|
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications
Xmod HF006SA is a high melt flow PP homopolymer with increased crystallinity, intended for injection molding. Xmod HF006SA is specifically developed for applications demanding a high surface appear..
|
|||
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179 |
|
Vyncolit 4421 XB Novolac Phenolic
Mineral and organic filled phenolic molding compound with good mechanical properties.USES: Fuse holders, brush holders, circuit breakers, automotive ignition and solenoid covers.Information provided..
|
|||
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | |
|
Arkema Group Nakan® RMS 501 L PVC, Rigid Injection Molding Grade
NAKAN RMS 501 L is a rigid polyvinyl chloride compound developed for injection molding of electrical boxes ( inside ).ISO data provided by the manufacturer, Arkema.
|
|||
| Charpy Impact, Notched |
0.250
J/cm² <br>@Temperature -30.0 °C
|
1.19
ft-lb/in² <br>@Temperature -22.0 °F
|
|
|
BASF Novolen® 2340 P Polypropylene
Grade with nucleating agent for injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | |
|
Arkema Group Appryl® HXN 1240 Polypropylene, 40% Talc Filled
Compound of a PP homopolymer and 40% talc, warm stabilized suitable for under hood automotive applications.ISO data provided by the manufacturer, Arkema.
|
|||
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | Conditioned; ISO 179/IeA |
|
Addiplast Addilene J 490 M40S Flame Retardant Polypropylene, 40% Mineral Filled
Flame retardant, mineral filled, with halogensInformation provided by Addiplast.
|
|||
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179-1/1eA |
|
Murtfeldt Murylat® SP Polyethylene Terephthalate
Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri..
|
|||
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179/IeA |
|
Addiplast Addilene H 442 M30 Polypropylene Homopolymer
High heat resistance, detergent stabilizedInformation provided by Addiplast.
|
|||
| Charpy Impact, Notched |
>=
0.250
J/cm² <br>@Temperature 23.0 °C
|
>=
1.19
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
PolyOne Gravi-Tech™ GRV-NY-060-CU Polyamide 6 (Nylon 6)
Information provided by PolyOne
|
|||
| Charpy Impact, Notched | 0.250 - 0.350 J/cm² | 1.19 - 1.67 ft-lb/in² | Compression; ISO 179/1eA |
|
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc..
|
|||
| Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | |
|
Arkema Group Oroglas® V 045 I Acrylic, Extrusion Grade
(discontinued **)
OROGLAS V 045 I is an extrusion that exhibits the following properties : 50% tougher than standard acrylics excellent optical properties ( comparable to that of standard acrylics) superior surface ..
|
|||
| Charpy Impact, Notched |
0.250
J/cm² <br>@Temperature 23.0 °C
|
1.19
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179-1/2 eA |
|
Hexion Bakelite™ PF 4010 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage
(disconti
Glass fiber reinforced and inorganically filled molding compound. High heat resistance, reduced molding shrinkage, good chemical resistance and mechanical properties.Application areas: Switch housi..
|
|||
| Charpy Impact, Notched | 0.250 - 1.50 J/cm² | 1.19 - 7.14 ft-lb/in² | Average value: 0.882 J/cm² Grade Count:11 |
|
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..
|
|||