| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature 23.0 °C
|
3.33
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB POLYfill PPH GF15030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature -30.0 °C
|
3.33
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® 513RS PC (Europe-Africa-Middle East)
LEXAN 513RS is a medium viscosity, glass reinforced, flame retardant grade UV stabilized grade.
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature -30.0 °C
|
3.33
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Asia Pacific)
Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
|
|||
| Charpy Impact, Notched | 0.700 - 1.20 J/cm² | 3.33 - 5.71 ft-lb/in² | Average value: 0.896 J/cm² Grade Count:13 |
|
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
|
|||
| Charpy Impact, Notched | 0.700 - 1.20 J/cm² | 3.33 - 5.71 ft-lb/in² | Average value: 0.900 J/cm² Grade Count:7 |
|
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179 1eA |
|
Lehmann & Voss LUVOCOM® 19-7342 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179 1eA |
|
Lehmann & Voss LUVOCOM® 19-7660 Polyamide 46, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot..
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179 |
|
Lucite International Perspexâ„¢ XT IM60 Acrylic Impact Modified Extruded Sheet
PERSPEX extruded sheet has a lower molecular weight making it easy to vacuum form and the extrusion process gives excellent thickness tolerance and is economical for long production runs.Information..
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics ULTEM CRS5011R PEI
Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179/2C |
|
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, ..
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature 23.0 °C
|
3.33
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Borealis BS4641 High Density Polyethylene
BS4641 is a bimodal high-density polyethylene homopolymer. Because of its excellent organoleptic properties, this grade is especially suitable for blow molding of bottles for food applications. App..
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179/1eA |
|
Borealis Xmod™ K65G2 20% Glass Fiber Reinforced Polypropylene Compound
Xmod K65G2 is a 20% glass fiber reinforced grade intended for injection molding. Xmod K65G2 has been developed especially for the car industry, to be used UTB parts. Xmod K65G2 offers good balance..
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature 23.0 °C
|
3.33
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
CP-Polymer-Technik Wellamid® 6000 GS 50 HWUVCP 50% Glass Sphere Filled Nylon 6, UV Stabilized, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | conditioned; ISO 179/1eA |
|
EMS-Grivory Grivory® GC-4H PA*-CF40
Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo..
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature 30.0 °C
|
3.33
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® HT XE 3996 PA*-GF30
Product description: Grivory XE 3996 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO-Polymer designatio..
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | conditioned; ISO 179/1eA |
|
EMS-Grivory Grivory® L 20 G HL PA12
Product Description: Grilamid L 20 GHL is a, medium viscosity injection molding grade, based on Polyamide 12 (PA12). Grilamid L 20 GHL is UV-stabilized, and heat stabilized The special features of G..
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature -30.0 °C
|
3.33
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
DuPont Performance Polymers Crastin® LW9030 BK851 PBT+ASA
(Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 BK851 is a 30% glass fiber reinforced black polybutylene terephthalate blend for injection mol..
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179/1eA |
|
DuPont Performance Polymers Crastin® LW9320LM BK591 PBT+SAN
(Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It ha..
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature -30.0 °C
|
3.33
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
DuPont Performance Polymers Delrin® 500T BK602 Acetal (POM)
(Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T BK602 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179/1eA |
|
DuPont Performance Polymers Delrin® SC699 NC010 Acetal (POM)
(Unverified Data**)
Silicone Lubricated Low Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry Delrin SC699 is a low viscosity acetal homopolymer lubricated developed for ..
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | DAM; ISO 179/1eA |
|
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**)
32% Mineral Reinforced Toughened Polyamide 66 Minlon 12TA BKB124 is a 32% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont P..
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature 30.0 °C
|
3.33
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® HT XE 4027 nat PA*-GF30
Product description: Grivory XE 4027 natural is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamid..
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature 30.0 °C
|
3.33
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® HT1V-3 FWA black 9225 PA6T/6I-GF30
Product description: Grivory HT1V-3 FWA black 9225 is a 30 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature 30.0 °C
|
3.33
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® HT1V-3 FWA nat PA6T/6I-GF30
Product description: Grivory HT1V-3 FWA natural is a 30 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6..
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179-1eA |
|
Barlog Plastics KEBATRON C1065X1 PPS, cross-linked, 65% glass fiber / mineral reinforced
PPS-GF/MD 65Information provided by BARLOG plastics GmbH.
|
|||
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | |
|
BASF Novolen® 2309 L Polypropylene
Cast film and thermoformed partsData was collected by ISO methods and provided by BASF.
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature -30.0 °C
|
3.33
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
BASF Ultrason E 1010 PES
Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability.
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature 23.0 °C
|
3.33
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB POLYfill PPHC K9030 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.700
J/cm² <br>@Temperature 30.0 °C
|
3.33
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30