| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -40.0 °C
|
3.81
ft-lb/in² <br>@Temperature -40.0 °F
|
DIN 53453 |
|
Nilit FRIANYL A63 TF10 Nylon 6.6 for injection molding, 10% PTFE lubricated
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179-1/1eA |
|
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data)
Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, ..
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
|
Covestro Apec® DP 1-9359/7 Polycarbonate
(discontinued **)
Key Features:Release agentUnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer M..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
DAM; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® FE270050 BK099 Nylon 66
(Unverified Data**)
Zytel® FE270050 BK099 is a 30% glass reinforced, polyamide 66 resin for gas and water assisted injection molding.Information provided by DuPont
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179 1eA |
|
Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
|
LATI Latilub 66-20T G/20-V1 PA66, 20% Glass Fiber Reinforced, PTFE Filled, Flame Retardant
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Euro..
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
|
LATI Latiohm 66-07 PD08 G/30 PA66, 30% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/2C |
|
SABIC Innovative Plastics ULTEM 4000 PEI (Europe-Africa-Middle East)
Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing.
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/2C |
|
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East)
VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications.
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Styrolution Terluran® GP-22 ABS
Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Europe-Africa-Middle East)
>PPE+PA66-I-TD10
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Unipetrol PE HD LITEN® MB/ML 67 HDPE
Made for injection molding applications.Information provided by Unipetrol RPA
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179 |
|
Total PPC 9760 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 9760 is heterophasic copolymer. PPC 9760 is characterized by improved stiffness, creep resistance and high impact resistance.
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eA |
|
Borealis Borpact™ SE920MO Polypropylene Homopolymer for Injection Molding
Borpact SE920MO is a high impact and transparent polypropylene. Borpact SE920MO is a new generation polypropylene having properties that were earlier not possible to combine. Borpact SE920MO offers..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
dry; ISO 179/1eA |
|
DSM Stanyl® TQ261F2 PA46-GF10
10% Glass Reinforced, Heat Stabilized
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | conditioned; ISO 179/1eA |
|
EMS-Grivory Grivory® GTR 45 PA6I/6T
Product description: Grivory GTR 45 is a transparent engineering thermoplastic based on amorphous, partially aromatic copolyamide for injection molding. Compared to other semi crystalline polyamides..
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | dry; ISO 179/1eA |
|
EMS-Grivory Grivory® HTV-4H1 nat PA6T/6I-GF40
Product description: Grivory HTV-4H1 natural is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac..
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | conditioned; ISO 179/1eA |
|
EMS-Grivory Grivory® HTV-4H1 nat PA6T/6I-GF40
Product description: Grivory HTV-4H1 natural is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac..
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | conditioned; ISO 179/1eA |
|
EMS-Grivory Grivory® LM-05 HX nat PA12
Product description: Grilamid LM-05 HX natural is a medium viscosity, heat-stabilized nanocomposite PA12 extrusion and injection molding grade. The special features of Grilamid LM-05 HX natural are:..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 30.0 °C
|
3.81
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® XE 3959 black 9992 PA610
Product description: Grilamid XE 3959 is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materials and i..
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | conditioned; ISO 179/1eA |
|
EMS-Grivory Grivory® XE 4028 nat PA12/MACMI
Product description: Grilamid XE 4028 natural is a transparent thermoplastic polyamides based on aliphatic, cycloaliphatic and aromatic blocks. Grilamid XE 4028 natural offers a variety of interesti..
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eA |
|
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)
(Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro..
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | conditioned; ISO 179/1eA |
|
EMS-Grivory Grivory® HT2C-3X black 9833 PA6T/66-CF30
Product description: Grivory HT2C-3X black 9833 us a 30% carbon-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc to ISO: PA 6T/66...
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179-1eA |
|
Barlog Plastics KEBATER A9030 PBT, 30% glass fiber reinforced, improved surface quality, reduced warpage
(PBT+X)-GF30Information provided by BARLOG plastics GmbH.
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
|
BASF Novolen® 2600 TC Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eA |
|
BASF Ultradur® S 4090 GX 14% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab..
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/IeA |
|
Addiplast Addilene H 511 V30 Polypropylene Homopolymer
Glass fiber reinforced, high modulus and improved stiffnessInformation provided by Addiplast.
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO179 |
|
Beijing Chemical Industry KAIFA® 301-G20 PBT Resin
20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
|
Covestro Apec® 1805 Polycarbonate
(discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation pr..
|
|||