| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
0.900
J/cm² @Temperature -30.0 °C |
4.28
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant.
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | DIN 53453 |
|
Nilit FRIANYL B63 H-TF20 Nylon 6 for injection molding, 20% PTFE lubricated
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | |
|
Polimeri Europa EDISTIR PD RR745E High Impact Polystyrene (HIPS)
(discontinued **)
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,G,088-03-07-12 Environmental stress cracking resistant (ESCR) HIPS. It combines high impact strength with high chemical r..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² @Temperature -30.0 °C |
4.28
ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
|
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² @Temperature -30.0 °C |
4.28
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER (Europe-Africa-Middle East)
Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and ..
|
|||
| Charpy Impact, Notched | 0.900 - 5.00 J/cm² | 4.28 - 23.8 ft-lb/in² | Average value: 2.57 J/cm² Grade Count:19 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Valox® 8032UX PBT+PET
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Valox® 830F PBT+PET
PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications
|
|||
| Charpy Impact, Notched |
0.900
J/cm² @Temperature -30.0 °C |
4.28
ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
|
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
|
|||
| Charpy Impact, Notched |
0.900
J/cm² @Temperature -30.0 °C |
4.28
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 (Europe-Africa-Middle East)
Heat stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin.
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO Data, Low Temp |
|
Styron Magnumâ„¢ 541 ABS, High Impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO Data, Low Temp |
|
Styron Magnumâ„¢ FG960 ABS, High Impact
MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS ..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | dry; ISO 179 |
|
Ter Hell Plastic Terez® PA 6 7750 TK Polyamide 6
Description: Medium viscosity, high impact modified standard grade PA 6, with crystallization accelerator and good flowability.Application: For molding parts with high impact stress.Information pr..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² @Temperature 30.0 °C |
4.28
ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® BG-25 HM PA6-GF25
Product description: Grilon BG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 25% glass fibers. Grilon BG-25 HM has the following important prop..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² @Temperature 30.0 °C |
4.28
ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® BG-30 HM PA6-GF30
Product description: Grilon BG-30 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 30% glass fibers. Grilon BG-30 HM has the following important prop..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² @Temperature 30.0 °C |
4.28
ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30
Product description: Grivory HT2V-3H is a 30 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamde. Polymer designation acc. to ISO: ..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² @Temperature 30.0 °C |
4.28
ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40
Product description: Grivory XE 4101 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179/1eA |
|
DuPont Performance Polymers Delrin® 500CL BK601 Acetal (POM)
(Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL BK601 is a medium viscosity acetal homopolymer containing a chemical lubricant designed for low wear and fr..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179/1eA |
|
DuPont Performance Polymers Delrin® PC650 NC010 Acetal (POM)
(Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC655 is a medium viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179/1eA |
|
DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² @Temperature -30.0 °C |
4.28
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² @Temperature 30.0 °C |
4.28
ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® XE 4217 black 9233 PA6T/66-GF45
Product description: Grivory XE 4217 black 9233 is a high heat stabilized, 45% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection moulding. Polymer designation..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179-1eA |
|
Barlog Plastics KEBATRON C2040G5 PPS, cross-linked, 40% GF, reduced residual chlorine
PPS-GF40Information provided by BARLOG plastics GmbH.
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179 |
|
BASF Petra® 130 BK-112 30% Glass Filled PET
Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength ..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179 |
|
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Conditioned)
Ultramid A 3HG2 is a 10% glass fiber reinforced grade of nylon 6/6 for injection molding.
|
|||