| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
1.20
J/cm² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® CE3510 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact, high heat and excellent extrusion and thermoforming characteristics. Halogen free..
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eA |
|
Nilit FRIANYL A63 GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact, Notched |
1.20
J/cm² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific)
Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB SCANAMID 66.6 C22^E F Nylon 66/6, Modified
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179-1/1eA |
|
Quadrant EPP Quadrant PPSU unfilled, extruded (ISO Data)
Quadrant PPSU is a black, amorphous high performance thermoplastic, offering better impact strength and chemical resistance than polysulfone and polyetherimide. Quadrant PPSU also has superior hydro..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® LI1911R PC (Europe-Africa-Middle East)
Low-viscosity multi-purpose grade having low levels of ionics species.
|
|||
| Charpy Impact, Notched |
1.20
J/cm² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® FXD171R PC (Europe-Africa-Middle East)
LEXAN FXD171R is a transparent/translucent high flow grade for light diffusion special effects. Color package may affect performance.
|
|||
| Charpy Impact, Notched |
1.20
-
1.60
J/cm² <br>@Thickness 3.00 - 3.00 mm
|
5.71
-
7.61
ft-lb/in² <br>@Thickness 0.118 - 0.118 in
|
Average value: 1.62 J/cm² Grade Count:4 |
|
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Grupo Repol Dinalon® A1S25 G35 H PA66 35% Glass Fiber, Heat Stabilized
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/2C |
|
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
|
|||
| Charpy Impact, Notched |
1.20
J/cm² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179 |
|
Teijin Multilon TN-7000F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. High stiffness realizes the thin wall of business machine chassis.Information provided by Teijin Chemicals Ltd.
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eA |
|
Styrolution Polystyrol 486 M GR 2 PS
Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys..
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eA |
|
Styron CALIBREâ„¢ 7100-8 Polycarbonate
CALIBREâ„¢ 7100-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eA |
|
Styron CALIBREâ„¢ 7102-8 Polycarbonate
CALIBREâ„¢ 7102-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eA |
|
Styron CALIBREâ„¢ 7103-8 Polycarbonate
CALIBREâ„¢ 7103-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO Data, Low Temp |
|
Styron Magnumâ„¢ 555 ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/2C |
|
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific)
Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT..
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eA |
|
Borealis Daplen™ MD206U Polypropylene Compound 20% Mineral Filled
Daplen MD206U is a 20% mineral filled polypropylene compound intended for injection molding. MD206U has been developed especially for automotive interior parts that require excellent balance betwee..
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | conditioned; ISO 179/1eA |
|
EMS-Grivory Grivory® AS/2 PA66
Product description: Grilon AS/2 is an unreinforced PA66 injection molding grade. Grilon AS/2 has the following important properties: Good flow behaviorEasy processingShort cycle times Grilon AS/2 i..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² <br>@Temperature 30.0 °C
|
5.71
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® B 70 GFE 30 H PA6-GF30
Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important p..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
CP-Polymer-Technik Wellamid® 6000 GVS 10/30 HWCP 10% Glass Fiber and 30% Glass Sphere Nylon 6, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Charpy Impact, Notched |
1.20
J/cm² <br>@Temperature -40.0 °C
|
5.71
ft-lb/in² <br>@Temperature -40.0 °F
|
50%RH; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per..
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | 50%RH; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | dry; ISO 179/1eA |
|
EMS-Grivory Grivory® LBV-65H FWA nat PA12-GF65
Product description: Grilamid LBV-65H FWA natural is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179 |
|
BASF Ultramid® N-333 NF3001 33% Glass Filled PA66 (Dry)
Ultramid N-333 NF3001 is a 33% glass reinforced, heat stabilized, injection molding
PA66 uncolored.
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/IeA |
|
Addiplast Addinyl PMD 20090 Nylon 6, 40% Glass Filled
Glass fiber reinforced, high resistance to frictionInformation provided by Addiplast.
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179 |
|
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Dry)
Ultramid 1503-2 NF2004 is a 33% glass reinforced, heat stabilized injection molding PA6/6.
|
|||
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | |
|
Ineos ABS NOVODUR® P3T ABS, Injection Grade
(discontinued **)
Injection molding grade, higher heat resistance.Applications: Automotive industry.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This grade was discontinued pri..
|
|||