Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/1eA
Nilit FRIANYL A63 HH-GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature -30.0 °C
6.19 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® RCY6713 PC (Asia Pacific)
Cycoloy* RCY6713 resin is an injection moldable high heat PC blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.5..
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific)
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature -30.0 °C
6.19 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS
Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses.
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East)
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature -30.0 °C
6.19 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD4472 PC
Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili..
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature -30.0 °C
6.19 ft-lb/in²
<br>@Temperature -22.0 °F
Ineos ABS Lustran® H701
Medium heat resistance, high impact strength. ,Property data per ISO test methods.
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature 23.0 °C
6.19 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Grupo Repol Dinalon® A1S25 G30 PA66 30% Glass Fiber
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, Conditioned
Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr..
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179
Teijin Panlite® L-1225ZL100 Transparent and Weather Resistant grade Polycarbonate Resin
Conforms to SAE regulations. It is a thin wall injection molding grade as it has high fluidity, weather resistance and mold release property and is bluish-tinted to exhibit clear color.Applications:..
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO Data, Low Temp
Styron CALIBREâ„¢ 300 10 Polycarbonate, General Purpose
CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren..
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO Data, Low Temp
Styron CALIBREâ„¢ MEGARAD 2080 10 Polycarbonate, Gamma Radiation Resistant
CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g..
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY
Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used..
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/1eU
DSM Stanyl® TE250F9 (DAM) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
Information provided by DSM Engineering Plastics.
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature -30.0 °C
6.19 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
DSM Stanyl® TE250F9 (DAM) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
Information provided by DSM Engineering Plastics.
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature 23.0 °C
6.19 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000/50 CP Nylon 6, Impact Modified Until 0°C, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® GV-4 FWA nat PA*-GF40
Product description: Grivory GV-4 FWA natural is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam..
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature 30.0 °C
6.19 ft-lb/in²
<br>@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® LV-65H SST nat PA12-GF65
Product description: Grilamid LV-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the foll..
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® XE 4174 black 9992 PA1010-GF30
Product description: Grilamid XE 4174 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4174 black 9992 are: PA1010..
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66 &nbsp;(Unverified Data**)
33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
Charpy Impact, Notched 1.30 - 1.70 J/cm²
6.19 - 8.09 ft-lb/in²
DIN 53 453
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced
These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also..
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature 30.0 °C
6.19 ft-lb/in²
<br>@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® GV-6H black PA*-GF60
Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature 30.0 °C
6.19 ft-lb/in²
<br>@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® L 25 W 40 NZ PA12-I
Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The..
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature -30.0 °C
6.19 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM) &nbsp;(Unverified Data**)
High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE NC010 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions...
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179-1eA
Barlog Plastics KEBAFORM C 908 EL POM Copolymer unreinforced, impact modified
POM-IInformation provided by BARLOG plastics GmbH.
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179
BASF Ultraform N 2640 Z4 UNC Q600 POM
Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade.
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature 23.0 °C
6.19 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature 23.0 °C
6.19 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Charpy Impact, Notched 1.30 J/cm²
<br>@Temperature -30.0 °C
6.19 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Lubrizol ESTALOC® 59003 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..