Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 1.40 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature -30.0 °C
6.66 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® 143R PC (Europe-Africa-Middle East)
LEXAN 143R is a medium viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 143R is available in transparent, translucent and opaque colours.
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature -30.0 °C
6.66 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® 164R PC (Europe-Africa-Middle East)
Medium viscosity, multi purpose polycarbonate resin with added release agent. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with b..
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature -30.0 °C
6.66 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® 955 PC (Europe-Africa-Middle East)
Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color..
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature -30.0 °C
6.66 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® 955AU PC (Europe-Africa-Middle East)
Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona..
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature 23.0 °C
6.66 ft-lb/in²
<br>@Temperature 73.4 °F
Radici Radilon® A RV300 990 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature -30.0 °C
6.66 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® FXD923A PC (Europe-Africa-Middle East)
LEXAN FXD923A is a transparent/translucent, medium viscosity, flame retardent grade for light diffusion special effects. UV-stabilized. Color package may affect performance.
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature -30.0 °C
6.66 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® FXE141R PC (Europe-Africa-Middle East)
LEXAN FXE141R is a medium viscosity multi purpose UV stabilized grade for visual effects in ""energy"". The material contains a release agent to ensure easy processing.
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature -30.0 °C
6.66 ft-lb/in²
<br>@Temperature -22.0 °F
ISO data
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Dry) &nbsp;(discontinued **)
Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with..
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature -30.0 °C
6.66 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® 950A PC (Europe-Africa-Middle East)
LEXAN 950A is a high viscosity flame retardant grade, especially suitable for electrical applications.
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO 179/1eA
Nilit FRIANYL B63 H-GV50 Nylon 6 for injection molding, 50% glass fiber reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO Data, Low Temp
Dow Isoplast® 2520 Polyurethane (PUR-RT), Impact Modified &nbsp;(discontinued **)
ISOPLAST® 2520 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include excel..
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO 179/1eA
Nilit FRIANYL B63 HS-GV10 Nylon 6 for injection molding, 10% glass fiber reinforced
Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 1.40 - 1.60 J/cm²
<br>@Thickness 3.00 - 3.00 mm
6.66 - 7.61 ft-lb/in²
<br>@Thickness 0.118 - 0.118 in
Average value: 1.55 J/cm² Grade Count:4
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature 23.0 °C
6.66 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000/42 CP Nylon 6, Polymer Modified, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO 179/1eU
DSM Stanyl® TW200F8 (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America)
Information provided by DSM Engineering Plastics.
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® GV-6 FWA black 9225 PA*-GF60
Product description: Grivory GV-6 FWA black 9225 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol..
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature -30.0 °C
6.66 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Delrin® 100TE NC010 Acetal (POM) &nbsp;(Unverified Data**)
Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100TE NC010 (formerly DE20580) is a high viscosity toughened acetal homopolymer with very low VOC emissions. Processing met..
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO 179-2
Denka CL-430 Transparent Resin Polymer (MABS) ABS
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® GV-6H black PA*-GF60
Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature 23.0 °C
6.66 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Akro-Plastic Akroloy® PA GF 40 (2845) PA 6.6 & PA6I/6T Conditioned, 40% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO 179
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Conditioned)
Ultramid 7423-2 NF3001 is an impact modified, 13% glass reinforced, heat stabilized injection molding PA6/6.
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO Data
BASF Capron® 8253 Impact Modified Nylon 6 (Dry) &nbsp;(discontinued **)
Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions..
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® GV-6H PA*-GF60
Product description: Grivory GV-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide...
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific)
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature 23.0 °C
6.66 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
BASF Ultramid® A3HG6 Balance 30% Glass Filled PA 66/610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..