| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
0.300
J/cm² <br>@Temperature -30.0 °C
|
1.43
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
Nilit FRIANYL A63 CV-CM 0515 9005/Z Powder-coatable nylon 6.6 for injection molding, 15% ceramic filled
Powder-coatable nylon 6.6 for injection molding, with conductive carbon blackInformation provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact, Notched |
0.300
J/cm² <br>@Temperature 23.0 °C
|
1.43
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB POLYfill PPH GK8040 Polypropylene Homopolymer, Glass Reinforced
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO Data |
|
Americas Styrenics Styron® 685P Polystyrene
(discontinued **)
STYRON® 685P general purpose polystyrene resin is a high heat resin with good strength, moldability/processability, and excellent clarity. This resin is typically used in consumer electronic applic..
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | |
|
Arkema Group Oroglas® MI-4T Acrylic, Heat Resistant
(discontinued **)
OROGLAS MI-4T is an acrylic grade that associates improved impact resistance with high heat resistance.Key features improved impact resistance: up to 4 times more impact resistant than standard acr..
|
|||
| Charpy Impact, Notched | 0.300 - 2.40 J/cm² | 1.43 - 11.4 ft-lb/in² | Average value: 0.904 J/cm² Grade Count:112 |
|
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
|
|||
| Charpy Impact, Notched |
0.300
-
0.460
J/cm² <br>@Temperature -30.0 - 30.0 °C
|
1.43
-
2.19
ft-lb/in² <br>@Temperature -22.0 - 86.0 °F
|
Average value: 0.380 J/cm² Grade Count:6 |
|
Overview of materials for Nylon 12, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179 1eA |
|
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Charpy Impact, Notched |
0.300
J/cm² <br>@Temperature 23.0 °C
|
1.43
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179-1/1eA |
|
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | |
|
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good surface appearance.Availability: Africa & Middle East; Asi..
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | |
|
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongationAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Amer..
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | 80*10*4mm, Cut; ISO 179/1eA |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 37T1020 PP
SABIC® PPcompound 37T1020 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits high impact and high flow, and is suitable for injection mold..
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179/1eA |
|
Solvay TECHNYL® C 52G4 MZ25 PA6, 25% mineral filler, DRY
Description: TECHNYL® C 52G4 MZ25 is a 25% mineral reinforced melamine cyanurate flame retarded polyamide 6.This product is heat stabilized and is suitable for injection molding. This product is ..
|
|||
| Charpy Impact, Notched |
0.300
J/cm² <br>@Temperature 23.0 °C
|
1.43
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Unipetrol PP MONSTEN® NB 218 Polypropylene Homopolymer
Made for fibers applications. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA
|
|||
| Charpy Impact, Notched |
0.300
J/cm² <br>@Temperature 23.0 °C
|
1.43
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Unipetrol PP MONSTEN® NB 425 Polypropylene Homopolymer
Made for non-woven textiles applications. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA
|
|||
| Charpy Impact, Notched |
0.300
J/cm² <br>@Temperature -20.0 °C
|
1.43
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179/1 |
|
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled
Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed..
|
|||
| Charpy Impact, Notched |
0.300
J/cm² <br>@Temperature 30.0 °C
|
1.43
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® AG-30 LF 15 PA66-(GF+Z)45
Product description: Grilon AG-30 LF 15 black 9832 is a heat stabilized, normal viscosity PA66 injection molding grade with 30% glass fibers and 15% of a combination of PTFE and silicone. Grilon AG-..
|
|||
| Charpy Impact, Notched |
0.300
J/cm² <br>@Temperature 30.0 °C
|
1.43
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® BGM-40 X PA6-(GF+MD)40
Product description: Grilon BGM-40 X is a heat stabilized PA 6 injection molding grade with a 40 % reinforcement combination (mineral and glass fiber). Grilon BGM-40 X has the following important pr..
|
|||
| Charpy Impact, Notched |
0.300
J/cm² <br>@Temperature -40.0 °C
|
1.43
ft-lb/in² <br>@Temperature -40.0 °F
|
50%RH; ISO 179/1eA |
|
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**)
32% Mineral Reinforced Toughened Polyamide 66 Minlon 12TA BKB124 is a 32% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont P..
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | dry; ISO 179/1eA |
|
EMS-Grivory Grivory® BGM-65 X V0 PA6-(GF+MD)65
Product description: Grilon BGM-65 X V0 is a flame retardant mineral and glass fiber reinforced PA6 injection molding grade. Grilon BGM-65 X V0 has the following important properties: Halogen and ph..
|
|||
| Charpy Impact, Notched |
0.300
J/cm² <br>@Temperature -30.0 °C
|
1.43
ft-lb/in² <br>@Temperature -22.0 °F
|
50%RH; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179/IeA |
|
Addiplast Addilene H 526 N30 Polypropylene Homopolymer
Improved rigidity, high durabilityInformation provided by Addiplast.
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179/IeA |
|
Addiplast Addinyl B2 E Flame Retardant Nylon 6
Flame retardant, halogen freeInformation provided by Addiplast.
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179/IeA |
|
Addiplast Addinyl B2 ZG30 Nylon 6, 30% Glass Bead
Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast.
|
|||
| Charpy Impact, Notched |
0.300
J/cm² <br>@Temperature 23.0 °C
|
1.43
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Arnite® A04 900 PET (European Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Charpy Impact, Notched | 0.300 - 1.50 J/cm² | 1.43 - 7.14 ft-lb/in² | Average value: 0.879 J/cm² Grade Count:37 |
|
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
|
|||
| Charpy Impact, Notched | 0.300 - 0.500 J/cm² | 1.43 - 2.38 ft-lb/in² | Average value: 0.433 J/cm² Grade Count:3 |
|
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
|
|||
| Charpy Impact, Notched | 0.300 - 0.500 J/cm² | 1.43 - 2.38 ft-lb/in² | Injection; ISO 179/1eA |
|
Raschig Group DECAL® 152CL Phenolic
Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet..
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | |
|
BASF Novolen® 1102 L Polypropylene
Data was collected by ISO methods and provided by BASF.
|
|||
| Charpy Impact, Notched | 0.300 J/cm² | 1.43 ft-lb/in² | ISO 179/1eA |
|
Polyplastics Duracon® CH-10 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||
| Charpy Impact, Notched |
0.300
J/cm² <br>@Temperature 30.0 °C
|
1.43
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® TS V0 PA666
Product description: Grilon TS V0 is an unreinforced, normal viscosity, self-extinguishing Polyamid 66 + Polyamide 6 injection molding grade. Grilon TS V0 is halogen free and free of red phosphorous..
|
|||