| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
0.350
J/cm² @Temperature 23.0 °C |
1.67
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
DuPont Performance Polymers Crastin® CE2055 NC010 PBT
(Unverified Data**)
Crastin® CE2055 NC010 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact, Notched | 0.350 - 1.10 J/cm² | 1.67 - 5.24 ft-lb/in² | Average value: 0.636 J/cm² Grade Count:12 |
|
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
|
|||
| Charpy Impact, Notched |
0.350
J/cm² @Temperature 23.0 °C |
1.67
ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
|
Polykemi AB POLYplex PMMA 700 Acrylic Glass
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.350
J/cm² @Temperature -30.0 °C |
1.67
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
Nilit FRIANYL A63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact, Notched |
0.350
-
4.50
J/cm² @Temperature -40.0 - 30.0 °C |
1.67
-
21.4
ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 1.39 J/cm² Grade Count:39 |
|
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
|
|||
| Charpy Impact, Notched |
0.350
J/cm² @Temperature -23.0 °C |
1.67
ft-lb/in² @Temperature -9.40 °F |
DIN 53453 |
|
Global PP-3370-RM Polypropylene Random Copolymer
Description-medium stiffness, low melting temperatures, very good for seal Applications-filmInformation provided by Global Polymers Corporation.
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | |
|
LATI Latishield 75/4-10A PBT, Steel Fiber Reinforced
EMI shielding product based on Polybutylene Terephthalate (PBT). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
|
Solvay TECHNYL® C 52G1 V25 Grey R7035 (XC 1329/A) PA6, DRY
Description: Polyamide 6, Glass-filled, glow-wire modified, color stabilized, lubricated for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Application..
|
|||
| Charpy Impact, Notched |
0.350
J/cm² @Temperature 23.0 °C |
1.67
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
Borealis HG385MO Polypropylene
HG385MO is a polypropylene homopolymer intended for injection molding. This grade combines unique Borstar® reactor design with Borstar® nucleation technology to produce highly-crystalline polyprop..
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
|
Polyplastics Duranex® CN7000 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179 |
|
Vyncolit X6151 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Highest impact, high strain to failure, glycol resistant.USES: Water pumps and water pump ..
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179-1 |
|
Vyncolit X7255 Glass Fiber Reinforced Novolac Phenolic
Novolac resin based, glass fiber and glass beads reinforced. Very easy to transform in complex shapes. Excellent mechanical and thermal properties. Higher isotropic properties and good dimensional s..
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179 |
|
Total PPH 10042 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 10042 is a nucleated antistatic homopolymer. PPH 10042 is characterized by high fluidity for high speed injection of thin wall articles such as dairy pots and tubs, salad ..
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
|
DuPont Performance Polymers Crastin® CE2055 NC010 Polybutylene Terephthalate (PBT)
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin CE2055 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Perf..
|
|||
| Charpy Impact, Notched |
0.350
J/cm² @Temperature -30.0 °C |
1.67
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)
20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage CharacteristicsCrastin SO653 NC010 is a 20% glass bead filled polybutylene terephthalate resin for injection molding. It has isotrop..
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/IeA |
|
Addiplast Addilene H 410 Polypropylene Homopolymer
UnreinforcedInformation provided by Addiplast.
|
|||
| Charpy Impact, Notched |
0.350
J/cm² @Temperature -30.0 °C |
1.67
ft-lb/in² @Temperature -22.0 °F |
|
|
BASF Novolen® 2600 TC Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
|
CENTROPLAST CENTROMID 6 G Polyamide 6 Cast
This material has good machinability and can be bonded or welded. Its applications include sliding bearings, hammerheads, and toothed gears.Information provided by CENTROPLAST Engineering Plastics ..
|
|||
| Charpy Impact, Notched |
0.350
J/cm² @Temperature -30.0 °C |
1.67
ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® FG151L NC010 Nylon 612
(Unverified Data**)
Unreinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179-1/1eA |
|
Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data)
This 30 % glass fibre reinforced grade offers higher stiffness, strength and creep resistance than the Duratron PAI grades mentioned above. It is well suited for structural applications supporting s..
|
|||
| Charpy Impact, Notched |
0.350
J/cm² @Temperature 23.0 °C |
1.67
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
Borealis HF136MO Polypropylene
HF136MO is a polypropylene homopolymer intended for injection molding. This grade is characterized by a good combination of mechanical and flow properties. This polymer is a CR (controlled rheology..
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
|
Polyplastics Duracon® KT-20 Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Wear resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||
| Charpy Impact, Notched |
0.350
J/cm² @Temperature 23.0 °C |
1.67
ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
|
Hexion Bakelite™ PF 6501 Phenolic Formaldehyde Resin, Low Shrinkage
Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant.Application areas: Thermally and dyna..
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179/1eA |
|
CENTROPLAST CENTRO HPM Polyetherimide
This material has high strength and rigidity at high temperatures, with good electrical properties. Applications include electrical insulators, and load-bearing components.Information provided by C..
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | Conditioned; ISO 179/IeA |
|
Addiplast Addilene PMD 50203 Flame Retardant Polypropylene
Flame retardant, unreinforced, with halogensInformation provided by Addiplast.
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | ISO 179-1/1eA |
|
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data)
Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte..
|
|||
| Charpy Impact, Notched |
0.350
J/cm² @Temperature 23.0 °C |
1.67
ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
|
Hexion Bakelite™ PF 4260 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength
Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistantApplication areas: Commutators (starte..
|
|||
| Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | |
|
LATI Kelon® A H CEG/40 PA 66, Glass/Mineral Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..
|
|||