| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
1.70
J/cm² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific)
Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | |
|
Polimeri Europa SINKRAL G320 ABS
(discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-25 General purpose injection moulding grade with good impact resistance, good flow and high gloss. SI..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179 1eA |
|
Lehmann & Voss LUVOCOM® 3/CF/30/EG Polyamide 6, with carbon fiber, extrusion grade
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179 |
|
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP
BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of ..
|
|||
| Charpy Impact, Notched |
1.70
J/cm² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
80x10x4mm, r=0.25; V-notch; ISO 179/1eA |
|
SYNTHOS Forsan® 573 L Acrylonitrile Butadiene Styrene (ABS)
Increased heat resistant, glossy, UV stabilized.Applications: Electrotechnics, automotiveHousehold appliances, office equipment, car interior parts, profiles, ABS sheets, etc.Synthos was formerly kn..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific)
DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179 |
|
Styrolution PS 495F HIPS
Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179 |
|
Styrolution Terluran® HH-106 ABS
Terluran HH-106 is an injection molding ABS grade with high resistance to heat deformation and impact.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics NORYL NH5120 PPE+PS
Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO Data |
|
Styron Magnumâ„¢ 341 ABS, Low Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics NORYL 731 PPE+PS
PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179/2C |
|
SABIC Innovative Plastics NORYL PX0844 PPE+PS
PPE+PS blend. Unfilled. UL94 HB rated. Low water absorption. Hydrolytic stability. Dimensional stability.
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Bayer Test |
|
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience ..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179/1eU |
|
DSM Stanyl® 46HF4130 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, High Flow (North America)
Information provided by DSM Engineering Plastics.
|
|||
| Charpy Impact, Notched |
1.70
J/cm² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | dry; ISO 179/1eA |
|
EMS-Grivory Grivory® XE 4105 nat PA610-GF50
Product description: Grilamid XE 4105 natural is a 50% glass fiber reinforced, heat stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | conditioned; ISO 179/1eA |
|
EMS-Grivory Grivory® XE 4107 nat PA612-GF40
Product description: Grilamid XE 4107 natural is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorptiong..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | conditioned; ISO 179/1eA |
|
EMS-Grivory Grivory® XE 4108 nat PA612-GF50
Product description: Grilamid XE 4108 natural is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorptiong..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | 50%RH; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66
(Unverified Data**)
33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | DAM; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**)
43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact, Notched |
1.70
J/cm² <br>@Temperature -30.0 °C
|
8.09
ft-lb/in² <br>@Temperature -22.0 °F
|
50%RH; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eA |
|
Eurostar Staramide PF00AS PA6, 50% Glass Fiber Filled, Injection Molded
Staramide PF00AS is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Charpy Impact, Notched |
1.70
J/cm² <br>@Temperature 23.0 °C
|
8.09
ft-lb/in² <br>@Temperature 73.4 °F
|
Dry; ISO 179/Af |
|
Arkema Group Orgalloy® RS 6600 Polyamide 6.6 Alloy
Polyamide Alloy, Rigid grade, Nylon 6.6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | |
|
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Dry)
Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | |
|
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO Data |
|
BASF Capron® 8333G HI HS BK-102 Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8333G HI HS BK-102 is a 33% glass reinforced, impact modified polyamide 6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughness in c..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | 80*10*4mm, Cut; ISO 179/1eA |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 5310 PP
SABIC® PPcompound 5310 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with exterior automotive weathering stability. The IMDS I..
|
|||
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics GELOY FXW751SK ASA+PC
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin
|
|||