Polymer Property : Charpy Impact, Notched = 2.38 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.500 J/cm²
<br>@Temperature -30.0 °C
2.38 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Nilit FRIANYL A63 SG15 Nylon 6.6 for injection molding, 15% mineral filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 SG-GV 2010 Nylon 6.6 for injection molding, 20% mineral filled and 10% glass fiber reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
DIN 53453
Nilit FRIANYL B63 KF20 Nylon 6 for injection molding, 20% short glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.500 J/cm²
<br>@Temperature 23.0 °C
2.38 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
Polykemi AB SCANMID 6 B12^ F20 NH6 Nylon 6, Glass Fiber Reinforced, Halogen Free, Flame Retardant
Information provided by Polykemi AB
Charpy Impact, Notched 0.500 - 0.900 J/cm²
2.38 - 4.28 ft-lb/in²
Average value: 0.765 J/cm² Grade Count:11
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 H Nylon 6.6 for injection molding
Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.500 J/cm²
<br>@Temperature 23.0 °C
2.38 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Victrex® PEEK 450FC30 General Purpose
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1U
Victrex® WG101™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai..
Charpy Impact, Notched 0.500 J/cm²
<br>@Temperature 23.0 °C
2.38 ft-lb/in²
<br>@Temperature 73.4 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66 &nbsp;(Unverified Data**)
Zytel® 103FHS BKB009 is a heat stabilized, internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Perf..
Charpy Impact, Notched 0.500 - 0.500 J/cm²
<br>@Temperature -30.0 - -30.0 °C
2.38 - 2.38 ft-lb/in²
<br>@Temperature -22.0 - -22.0 °F
Average value: 0.500 J/cm² Grade Count:1
Overview of materials for Nylon 66, Film
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East)
VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors.
Charpy Impact, Notched 0.500 J/cm²
<br>@Temperature -20.0 °C
2.38 ft-lb/in²
<br>@Temperature -4.00 °F
ISO 179/2C
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PA (Europe-Africa-Middle East)
NORYL GTX820 is a 20% glass reinforced grade with excellent chemical resistance in combination with high stiffness and heat resistance.
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East)
6.5% glass reinforced, Super High Flow, flame retardant PBT.
Charpy Impact, Notched 0.500 J/cm²
<br>@Temperature -20.0 °C
2.38 ft-lb/in²
<br>@Temperature -4.00 °F
ISO 179/1eA
Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets
Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® CN7015 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® BGM-40 X PA6-(GF+MD)40
Product description: Grilon BGM-40 X is a heat stabilized PA 6 injection molding grade with a 40 % reinforcement combination (mineral and glass fiber). Grilon BGM-40 X has the following important pr..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
DuPont Performance Polymers Crastin® SK601 BK851 Polybutylene Terephthalate (PBT) &nbsp;(Unverified Data**)
10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 BK851 is a 10% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
Conditioned; ISO 179/IeA
Addiplast Addinyl B2 ZG30 Nylon 6, 30% Glass Bead
Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast.
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
DIN 53453
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable..
Charpy Impact, Notched 0.500 - 0.600 J/cm²
<br>@Temperature -20.0 - -20.0 °C
2.38 - 2.86 ft-lb/in²
<br>@Temperature -4.00 - -4.00 °F
Average value: 0.550 J/cm² Grade Count:2
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Charpy Impact, Notched 0.500 J/cm²
<br>@Temperature 23.0 °C
2.38 ft-lb/in²
<br>@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® A 218 S30 Black 21 N PA66, 30% glass fiber, Conditioned
Description: Polyamide PA66, reinforced with 30% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 218 S30 is used in all sectors of indu..
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
IS0179-1:2000
Zhejiang Juner PA-A6-6H High CTI Value Halogen-Free Environmental Protection Flame-Resistant and Reinforced Polyamide
Applications: Circuit Breaker, BaseInformation provided by Zhejiang Juner New Materials Co, Ltd.