| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® 121 PC (Europe-Africa-Middle East)
LEXAN 121 is a low viscosity multi purpose grade available in transparent, translucent and opaque colours.
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® 121R PC (Asia Pacific)
Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release.
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® 123R PC (Europe-Africa-Middle East)
LEXAN 123R is a low viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 123R is available in transparent, translucent and opaque colours.
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® 124R PC (Europe-Africa-Middle East)
Low viscosity, multi purpose polycarbonate resin with added release agent. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bi..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® 223R PC (Europe-Africa-Middle East)
LEXAN 223R is a low viscosity, UV stabilized multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved.
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® 915AU PC (Asia Pacific)
LEXAN resin grade 915AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in transparent colors, inte..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® 915R PC (Europe-Africa-Middle East)
Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties...
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Asia Pacific)
Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ..
|
|||
| Charpy Impact, Notched |
6.50
J/cm² <br>@Temperature -30.0 °C
|
30.9
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
|
|||
| Charpy Impact, Notched |
6.50
J/cm² <br>@Temperature -30.0 °C
|
30.9
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Asia Pacific)
Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific)
Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL8454 PC COPOLYMER (Asia Pacific)
Lexan* EXL8454 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 50% post consumer recycle content. Limited availability and restricted color only. Higher color..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® FXD121 PC (Europe-Africa-Middle East)
Transparent/translucent PC for light diffusion special effects. Color package may affect performance.
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® HP1HF PC (Europe-Africa-Middle East)
Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable.
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® HP1R PC (Europe-Africa-Middle East)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount o..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® HP2R PC (Europe-Africa-Middle East)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a hi..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer
Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Asia Pacific)
Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® LUX2414G PC (Asia Pacific)
10 MFR. Improved flame retardance. Internal mold release. UV stabilized.
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/2C |
|
SABIC Innovative Plastics GELOY XTPM405 ASA+PC
High flow PC/ASA with improved impact at room and low temperatures. Improved release. Excellent weatherability for outdoor unpainted or clearcoated applications. Injection Moldable with large color ..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® 221R PC (Europe-Africa-Middle East)
LEXAN 221R is a low viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.4 mm approved.
|
|||
| Charpy Impact, Notched |
6.50
J/cm² <br>@Temperature -30.0 °C
|
30.9
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® HP2NR PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179 |
|
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP
SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are ..
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179-1 |
|
Unitika EX-1222 PA6, Dry
High-impact nylonInformation provided by Unitika Ltd.
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/1eA |
|
Covestro Makroblend® KU 2-7915 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradeexcellent toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content
|
|||
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | dry; ISO 179/1eA |
|
EMS-Grivory Grivory® BFZ 3 PA6
Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Gril..
|
|||