| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
Nilit FRIANYL A63 HH-TFGV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated, 30% glass fiber reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179/1eA |
|
Nilit FRIANYL A63 S Nylon 6.6 for injection molding
Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER (Europe-Africa-Middle East)
Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm ..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East)
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics GELOY CR7501 ASA (Europe-Africa-Middle East)
High heat injection moulding grade, blend of ASA/AMSAN. It can be positioned for outside parts in various markets. Various colours.
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179 |
|
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66
Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179-1/1eA |
|
Quadrant EPP Quadrant PC 1000 extruded (ISO Data)
Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra..
|
|||
| Charpy Impact, Notched | 0.900 - 1.80 J/cm² | 4.28 - 8.57 ft-lb/in² | Average value: 1.35 J/cm² Grade Count:6 |
|
Overview of materials for Nylon, Amorphous Transparent Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature 23.0 °C
|
4.28
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Grupo Repol Dinalon® A1S25 G25 PA66 25% Glass Fiber
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179 1eA |
|
Lehmann & Voss LUVOCOM® 1100/GF/30/NAT Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179/2C |
|
SABIC Innovative Plastics ULTEM 2210R PEI (Europe-Africa-Middle East)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics NORYL IGN5531 PPE+PS
Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East)
VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin.
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 (Europe-Africa-Middle East)
UV stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin.
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature 23.0 °C
|
4.28
ft-lb/in² <br>@Temperature 73.4 °F
|
dry; ISO 179/1eA |
|
DSM Akulon® N24-G6 PA6-GF30
30% Glass Reinforced
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature 23.0 °C
|
4.28
ft-lb/in² <br>@Temperature 73.4 °F
|
dry; ISO 179/1eA |
|
DSM Akulon® SG-KGS6 PA66-GF30 FR
30% Glass Reinforced, Halogen free and free of red phosphorous
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eU |
|
DSM Stanyl® TW341 (DAM) Nylon 46 Heat Stabilized, Lubricated (North America)
Information provided by DSM Engineering Plastics.
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature 30.0 °C
|
4.28
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® XE 3982 PA12
Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature -40.0 °C
|
4.28
ft-lb/in² <br>@Temperature -40.0 °F
|
DAM; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**)
35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR NC010 is a 35% glass reinforced toughened heat stabilized lubricated high performance polyamide resin. It is also a P..
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature 30.0 °C
|
4.28
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® TR 90 UV PAMACM12
Product description: Grilamid TR 90 UV natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid 90 UV natural offers outstanding propert..
|
|||
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179 |
|
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
High FDI; high heat
|
|||
| Charpy Impact, Notched |
0.900
J/cm² <br>@Temperature -30.0 °C
|
4.28
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics NORYL FE1630PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1630PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
|
|||