Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO179/3C DIN.53453
Omnia Plastica Akulon® POM h Acetal Homopolymer
The general features of homopolymer acetalic resin are similar to those of copolymer POM c, except that service temperature (under load) is slightly higher but resistance to hydrolysis and strong al..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper..
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO 179
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO 179/1eA
Nilit FRIANYL A63 H-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.24 ft-lb/in²

@Temperature 73.4 °F
ASTM D256
Qualchem Danaprop PP2GF-15 Polypropylene, 15% Glass Fiber
Polypropylene (homo-polymer) reinforced with glass fiberInformation provided by Qualchem Zrt.
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
DIN 53453
Nilit FRIANYL C73 TFGV1530 Nylon 6.6/6 for injection molding, 15% PTFE lubricated, 30% glass fiber reinforced
Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 1.10 - 4.50 J/cm²

@Temperature -30.0 - 30.0 °C
5.24 - 21.4 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 3.03 J/cm² Grade Count:8
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Charpy Impact, Notched >= 1.10 J/cm²

@Temperature 23.0 °C
>= 5.24 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Grupo Repol Dinalon® B1S25 G30PV0 30% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 6
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
Eastman Ecdel PCCE 9965 Copolyester Ether Elastomer
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.24 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000/42 Nylon 6, Polymer Modified, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.24 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 GV 15 HWCP 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.24 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600/506 HWCP Nylon 66, Impact Modified, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO 179
Chi Mei Polylac® PA-707 ABS
High gloss, high rigid
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO 179
Chi Mei Polylac® PA-756 ABS - High Flow
High rigid, high flow
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO 179
Chi Mei Polylac® PA-777E ABS - High Heat
Ultra High Heat
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
Arkema Group Nakan® RPS 400 M PVC, Rigid Extrusion Grade
NAKAN RPS 400 M is a rigid polyvinyl chloride compound developed for extrusion of cables ducts.ISO data provided by the manufacturer, Arkema.
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BMF Nylon 11 (Dry)
Designation ISO 1874-PA11,M,12-010Rigid grade for injection molding. Available color: natural. Additive free.Good melt viscosity. Outstanding ability to mold part with high length-thickness ratio an..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
BASF Luranyl® KR 2454/3 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced
Heat resistant grade with halogen-free flame retardant; applications include TV plug connectors and components in switchgear cabinets.Data was collected by ISO methods and provided by BASF.
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO 179
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Dry)
Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6.
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO 179
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Conditioned)
Ultramid 1703-2 BK ND3007 is a 25% glass reinforced, heat stabilized injection molding nylon 6/6.
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO 179/1eA
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Conditioned)
Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability.
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
ISO data
BASF Capron® 8333G HI HS BK-102 Impact Modified, 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8333G HI HS BK-102 is a 33% glass reinforced, impact modified polyamide 6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughness in c..
Charpy Impact, Notched 1.10 - 1.40 J/cm²

@Temperature -30.0 - -30.0 °C
5.24 - 6.66 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.24 J/cm² Grade Count:5
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is ..
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO179
Beijing Chemical Industry KAIFA® MN201-G20 Nylon 66 Resin
20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO 179/1eA
BASF Ultradur B 4300 G6 30% Glass Filled PBT
Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® HP25X Acetal Co-polymer (POM), High stiffness, High viscosity
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..