| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Asia Pacific)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
|
|||
| Charpy Impact, Notched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
|
|||
| Charpy Impact, Notched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
|
|||
| Charpy Impact, Notched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.
|
|||
| Charpy Impact, Notched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL9330P PC COPOLYMER (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA.
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® HF1110R PC (Europe-Africa-Middle East)
LEXAN HF1110R is a high flow grade especially designed for applications that require thin wall sections and high flow lengths.
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® HF1140R PC (Europe-Africa-Middle East)
LEXAN HF1140R is a high flow grade. This material is especially designed for applications that require thin wall sections and high flow lengths. FDA food contact compliant in limited colors.Effect..
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® HPS1R PC (Europe-Africa-Middle East)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains..
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® ML7647 PC (Asia Pacific)
Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Europe-Africa-Middle East)
Cycoloy Medium Heat Plating Grade for Automotive
|
|||
| Charpy Impact, Notched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Asia Pacific)
Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
|
|||
| Charpy Impact, Notched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer
Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af..
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® FXR123R PC (Europe-Africa-Middle East)
Lexan FXR123R Resin
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Xenoy® X4820 PBT+PC
Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability.
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific)
Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability.
|
|||
| Charpy Impact, Notched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics LNP Thermocomp ML4351HF PC (Asia Pacific)
LNP* Thermocomp* ML4351HF is a Light Reflecting Grade.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | IS0179-1:2000 |
|
Zhejiang Juner PC-A1 Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | IS0179-1:2000 |
|
Zhejiang Juner PC-A2-1 Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | IS0179-1:2000 |
|
Zhejiang Juner PC-A2-10 Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | IS0179-1:2000 |
|
Zhejiang Juner PC-A2 Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1eA |
|
Covestro Makroblend® KU 2-7912 MBS151 Polycarbonate + PBT, Impact Grade
(PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedAs of 1 September 2015, Bayer MaterialScience was separated..
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | dry; ISO 179/1eA |
|
EMS-Grivory Grivory® BZ 3 PA6
Information provided by EMS Grivory
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1eA |
|
Covestro Makroblend® KU 2-7912 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedPreprocessingMax. Water content
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | IS0179-1:2000 |
|
Zhejiang Juner PC-A1-10 Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | IS0179-1:2000 |
|
Zhejiang Juner PC-A1-18 Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
|
|||
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® ML3485 PC (Europe-Africa-Middle East)
LEXAN ML3485 is a low viscosity grade exhibiting an improved ductility over standard polycarbonate grades at equal flow.
|
|||