Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature 23.0 °C
8.09 ft-lb/in²
<br>@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature -30.0 °C
8.09 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics GELOY HRA170D ASA+PC (Europe-Africa-Middle East)
GELOY HRA170D resin is a PC-ASA blend with permanent antistatic behavior. It is typically used in applications that require antidust properties and high impact retention. Geloy HRA170D resin is typi..
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature -30.0 °C
8.09 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer
Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in..
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature 23.0 °C
8.09 ft-lb/in²
<br>@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer
High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regi..
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature 23.0 °C
8.09 ft-lb/in²
<br>@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacifi..
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
Ineos ABS Lustran® H605
Low emission, easy flowing.,Property data per ISO test methods.
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179/1eA
Kuraray Genestarâ„¢ G1301A-M61 Nylon, 30% Glass Filled
30% Glass reinforced and impact modified injection grade.Main Features:Higher elongation and impact strengthHeat resistanceChemical resistanceExample of applications:Quick connector
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179/1eA
Kuraray Genestarâ„¢ G1500A-M61 Nylon, 50% Glass Filled
50% Glass reinforced injection grade. Main Features:High strengthHeat resistanceExamples of applications:Structural partsSteel alternating parts
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off..
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific)
DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, Conditioned
Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used..
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics NORYL NH5120C PPE+PS
Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The ..
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics NORYL 725A PPE+HIPS (Europe-Africa-Middle East)
NORYL 725A is an unfilled material, with a Vicat B/120 of 135°C according ISO 306. NORYL 725A has been designed for use in automotive interior applications, where anti-squeak is required.
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature 23.0 °C
8.09 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 HWCP Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature 23.0 °C
8.09 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 HWUVCP Nylon 66, UV Stabilized, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature 23.0 °C
8.09 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 PA-66-HWV0CP UL-Licensed Nylon 66, Flame Protection, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® TSGZ-15 PA666-GF15
Product description: Grilon TSGZ-15 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 15% glass fibers. Grilon TSGZ-15 has the following important p..
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® XE 4104 nat PA610-GF40
Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia..
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® XE 4108 nat PA612-GF50
Product description: Grilamid XE 4108 natural is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorptiong..
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature -30.0 °C
8.09 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Delrin® 100STE NC010 Acetal (POM) &nbsp;(Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100STE NC010 (formerly DE20590) is a high-viscosity super-toughened acetal homopolymer with very low VOC emissions. P..
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature -30.0 °C
8.09 ft-lb/in²
<br>@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® ST801AHS BK010 Nylon 66 &nbsp;(Unverified Data**)
Super Toughened Heat Stabilized Polyamide 66 Zytel ST801AHS BK010 is a Super Tough high performance black polyamide 66 resin. It offers outstanding molding performance in injection molding applicati..
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature -30.0 °C
8.09 ft-lb/in²
<br>@Temperature -22.0 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66 &nbsp;(Unverified Data**)
Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature -30.0 °C
8.09 ft-lb/in²
<br>@Temperature -22.0 °F
BASF Novolen® 2900 H Polypropylene
Injection molded and thermoformed parts.Data was collected by ISO methods and provided by BASF.
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature 23.0 °C
8.09 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature 23.0 °C
8.09 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics NORYL PX2355 PPE+HIPS (Europe-Africa-Middle East)
NORYL PX2355 is an unfilled, medium heat, low odour and low emission material with excellent heat aging performance. It has been developed for automotive interior applications, such as instrument pa..
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature -30.0 °C
8.09 ft-lb/in²
<br>@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6 &nbsp;(Unverified Data**)
40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex..
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
Polimeri Europa SINKRAL C423/M3 ABS &nbsp;(discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,95-08-16-15 Special low gloss grade for injection moulding. Good impact resistance coupled with good flow permi..