Polymer Property : Charpy Impact, Notched = 8.09 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.130 - 1.70 J/cm²
<br>@Temperature -30.0 - 10.0 °C
0.619 - 8.09 ft-lb/in²
<br>@Temperature -22.0 - 50.0 °F
Average value: 0.367 J/cm² Grade Count:85
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Charpy Impact, Notched 0.400 - 1.70 J/cm²
1.90 - 8.09 ft-lb/in²
Average value: 0.885 J/cm² Grade Count:17
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Charpy Impact, Notched 0.200 - 1.70 J/cm²
0.952 - 8.09 ft-lb/in²
Average value: 0.635 J/cm² Grade Count:40
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Charpy Impact, Notched 0.300 - 1.70 J/cm²
<br>@Temperature -40.0 - 30.0 °C
1.43 - 8.09 ft-lb/in²
<br>@Temperature -40.0 - 86.0 °F
Average value: 1.07 J/cm² Grade Count:22
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Charpy Impact, Notched 0.600 - 1.70 J/cm²
<br>@Temperature -30.0 - 0.000 °C
2.86 - 8.09 ft-lb/in²
<br>@Temperature -22.0 - 32.0 °F
Average value: 1.24 J/cm² Grade Count:6
Overview of materials for Nylon, Amorphous Transparent Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value..
Charpy Impact, Notched 1.30 - 1.70 J/cm²
6.19 - 8.09 ft-lb/in²
DIN 53 453
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced
These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also..