| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | dry; ISO 179-1/1eA |
|
Murtfeldt Murdopol® Nylon 12
Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f..
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179 |
|
PolyOne OnForce™ LFT PP-40LGF/001 UV Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS
Reinforced PC/ABS with high stiffness and low CTE.
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179/1eA |
|
Nilit FRIANYL B63 L-HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced
Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact, Notched |
2.00
J/cm² <br>@Temperature 23.0 °C
|
9.52
ft-lb/in² <br>@Temperature 73.4 °F
|
|
|
Radici Radilon® S RV300R (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific)
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
|
|||
| Charpy Impact, Notched |
2.00
-
5.50
J/cm² <br>@Temperature -30.0 - -30.0 °C
|
9.52
-
26.2
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 3.50 J/cm² Grade Count:5 |
|
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
|
|||
| Charpy Impact, Notched |
2.00
J/cm² <br>@Temperature -30.0 °C
|
9.52
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 eA |
|
Lehmann & Voss LUVOCOM® 50-0828 Polycarbonate, with glass fiber, PTFE, lubricant modified
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics NORYL SE90 PPE+HIPS (Europe-Africa-Middle East)
NORYL SE90 is an unfilled, flame retardant material with a Vicat B/120 of 110°C according ISO 306. NORYL SE90 is V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815.
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179/1eA |
|
Solvay TECHNYL® C 216 V45 PA6, 45% glass fiber, Conditioned
Description: Polyamide PA6, reinforced with 45% of glass fiber, for injection molding.Available in: EuropeProduct Applications: TECHNYL C 216 V45 has been optimized to have high impact strength, a n..
|
|||
| Charpy Impact, Notched |
2.00
J/cm² <br>@Temperature -30.0 °C
|
9.52
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/2C |
|
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East)
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..
|
|||
| Charpy Impact, Notched |
2.00
J/cm² <br>@Temperature 23.0 °C
|
9.52
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Styron CALIBREâ„¢ 701-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 701-15 Series resins are formulated and produced to supply both clarity and enhanced ignition resistance. They do so while maintaining excellent physical properties and proce..
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO Data |
|
Styron Magnumâ„¢ 780HP ABS, High Heat, High Impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Asia Pacific)
NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance.
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179/1eA |
|
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled
Daplen EE137AI is a 10% mineral filled grade intended for injection molding. EE137AI has been developed especially for the car industry, to be used in interior parts where high scratch resistance i..
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179/1eA |
|
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled
Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed..
|
|||
| Charpy Impact, Notched |
2.00
J/cm² <br>@Temperature 30.0 °C
|
9.52
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® 1SVX-65H nat PA1010-GF65
Product Description: Grilamid 1SVX-65H natural is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E..
|
|||
| Charpy Impact, Notched |
2.00
J/cm² <br>@Temperature 30.0 °C
|
9.52
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® AZ 3 PA66
Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures..
|
|||
| Charpy Impact, Notched |
2.00
J/cm² <br>@Temperature 30.0 °C
|
9.52
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® LV-2A NZ PA12-GF20
Product description: Grilamid LV-2A NZ is a high viscosity polyamide 12 with 20% glass fibers and improved hydrolysis resistance compared to standard polyamide 12 materials. Grilamid LV-2A NZ has a ..
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | dry; ISO 179/1eA |
|
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55
Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint..
|
|||
| Charpy Impact, Notched |
2.00
J/cm² <br>@Temperature 30.0 °C
|
9.52
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® XE 4129 black 9020 PA610
Product description: Grilamid XE 4129 black 9020 is a high viscosity Polyamide 610 especially suitable for extrusion applications. A characteristic of tubes made out of this material is the high res..
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | dry; ISO 179/1eA |
|
EMS-Grivory Grivory® XE 5052 (BGZ-15 FC) PA6-GF15
Product description: Grilon XE 5052 is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber: High impact resistanceGood surface qualityShort cycle timeGood flowabilit..
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | After conditioning at 23°C/50%RH; ISO 179/Af |
|
Arkema Group Orgalloy® RS 6000 Polyamide 6 Alloy
Polyamide Alloy, Rigid grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | After conditioning at 23°C/50%RH; ISO 179/Af |
|
Arkema Group Orgalloy® RS 6600 Polyamide 6.6 Alloy
Polyamide Alloy, Rigid grade, Nylon 6.6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
|
|||
| Charpy Impact, Notched |
2.00
J/cm² <br>@Temperature -30.0 °C
|
9.52
ft-lb/in² <br>@Temperature -22.0 °F
|
|
|
BASF Luranyl® KR 2401 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade
Base grade with a balanced combination of impact strength and stiffness. Uses include: parts of vehicle interiors, air ducts and loudspeaker housings.Data was collected by ISO methods and provided ..
|
|||
| Charpy Impact, Notched |
2.00
J/cm² <br>@Temperature 23.0 °C
|
9.52
ft-lb/in² <br>@Temperature 73.4 °F
|
Dry; ISO 179/Af |
|
Arkema Group Orgalloy® RS 6010 Polyamide 6 Alloy 10% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group
|
|||
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | |
|
LATI Latiblend 7587 E61-V0 PBT/PC, Flame Retardant
Blend based on Polybutylene Terephthalate (PBT) / Polycarbonate (PC). Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. High impact re..
|
|||