Polymer Property : Izod Impact, Notched = 0.0937 ft-lb/in - NB Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.0500 J/cm - NB
0.0937 ft-lb/in - NB
Average value: 1.04 J/cm Grade Count:174
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched 0.0500 - 7.50 J/cm
<br>@Temperature -40.0 - 0.000 °C
0.0937 - 14.1 ft-lb/in
<br>@Temperature -40.0 - 32.0 °F
Average value: 2.43 J/cm Grade Count:55
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.0500 J/cm
0.0937 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant.
Izod Impact, Notched 0.0500 J/cm
0.0937 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated.
Izod Impact, Notched 0.0500 J/cm
0.0937 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer
LNP* LUBRICOMP* KL001 is a compound based on Acetal Copolymer resin containing 5% PTFE. Added feature of this material is: Wear Resistant.
Izod Impact, Notched 0.0500 J/cm
0.0937 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KL001 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched 0.0500 J/cm
0.0937 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT
LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant.
Izod Impact, Notched 0.0500 J/cm
<br>@Temperature -30.0 °C
0.0937 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
Izod Impact, Notched 0.0500 J/cm
<br>@Temperature -30.0 °C
0.0937 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Asia Pacific)
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
Izod Impact, Notched 0.0500 J/cm
<br>@Temperature -30.0 °C
0.0937 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East)
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
Izod Impact, Notched 0.0500 J/cm
<br>@Temperature 0.000 °C
0.0937 ft-lb/in
<br>@Temperature 32.0 °F
ASTM D256
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 0.0500 J/cm
<br>@Temperature 0.000 °C
0.0937 ft-lb/in
<br>@Temperature 32.0 °F
ASTM D256
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 0.0500 J/cm
<br>@Temperature 0.000 °C
0.0937 ft-lb/in
<br>@Temperature 32.0 °F
ASTM D256
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 0.0500 J/cm
<br>@Temperature 0.000 °C
0.0937 ft-lb/in
<br>@Temperature 32.0 °F
ASTM D256
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 0.0500 J/cm
<br>@Temperature 0.000 °C
0.0937 ft-lb/in
<br>@Temperature 32.0 °F
ASTM D256
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 0.0500 J/cm
<br>@Temperature 0.000 °C
0.0937 ft-lb/in
<br>@Temperature 32.0 °F
ASTM D256
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 0.0500 J/cm
<br>@Temperature 23.0 °C
0.0937 ft-lb/in
<br>@Temperature 73.4 °F
ISO 180/A
Cossa Polimeri ESTABLEND PA 1560 T8 GF ABS / Nylon 6 Blend, 30% Glass & Mineral Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.30% glass fiber and mineral fillerGood impact strength, high chemical resistance, excellent heat resistance, high dimension..