Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.180 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.180 J/cm
0.337 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycolac® INP563 ABS+SAN
SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Izod Impact, Notched 0.180 J/cm
0.337 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycolac® INPBMAT ABS
Cross-linked SAN in styrenic matrix. Provides excellent gloss reduction properties. Maintains original polymer properties such as impact etc. Compatible with various polymer such as PVC and ABS. C..
Izod Impact, Notched 0.180 - 2.14 J/cm
0.337 - 4.00 ft-lb/in
Average value: 0.563 J/cm Grade Count:25
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Izod Impact, Notched 0.180 J/cm
0.337 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in water-c..
Izod Impact, Notched 0.180 J/cm
0.337 ft-lb/in
ASTM D256
I. Stern GPPS-020 General Purpose Crystal Polystyrene
Features:High Strength GradeHigh Flow, High ToughnessExcellent ProcessabilityApplicationsInjection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co...
Izod Impact, Notched 0.180 J/cm
0.337 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in wat..
Izod Impact, Notched 0.180 J/cm
0.337 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester Elastomer
LNP THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Glass Fiber, Mineral. Added features of this material include: Flame Retardant.
Izod Impact, Notched 0.180 J/cm
<br>@Thickness 3.20 mm
0.337 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Supreme Petrochem SC 201E General Purpose Polystyrene
CharacteristicsVery high molecular weight High heat grade Good melt strength Good clarity and mechanical strengthProcessing Extrusion MoldingApplicationsExtruded embossed sheets, OPS, foamed meat t..
Izod Impact, Notched 0.180 J/cm
<br>@Thickness 3.20 mm
0.337 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Supreme Petrochem SC 208 General Purpose Polystyrene
CharacteristicsHigh flow grade Easy processing Good clarity & shineProcessing Extrusion MoldingApplications Hand molding applications of novelty items, toys etc. Carrier for master batches, as a ..
Izod Impact, Notched 0.180 J/cm
0.337 ft-lb/in
ASTM D256
Plenco 4466 Phenolic, Granular, Compression Molded
PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466..
Izod Impact, Notched 0.180 J/cm
0.337 ft-lb/in
ASTM D256
Plenco 5482 Phenolic, Granular, Transfer Molded
PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect..
Izod Impact, Notched 0.180 J/cm
<br>@Temperature 23.0 °C
0.337 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
Denka STYROL MW1 Polystyrene
"DENKA SYTROL MW" is a well-balanced polystyrene (PS) resin, with a high tensile strength as well as good moldability. Overturning the traditional understanding that PS resin is "hard and brittle," ..
Izod Impact, Notched 0.180 J/cm
<br>@Thickness 3.20 mm
0.337 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Beijing Chemical Industry KAIFA® GL1100 ABS General Purpose Grade
High gloss, excellent external appearanceInformation provided by Beijing Chemical Industry Research Institute (Group)
Izod Impact, Notched 0.180 J/cm
<br>@Thickness 3.20 mm
0.337 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Beijing Chemical Industry KAIFA® GL2100 ABS Good Flow Grade
Good flow, Easy processing, High glossInformation provided by Beijing Chemical Industry Research Institute (Group)
Izod Impact, Notched 0.180 J/cm
0.337 ft-lb/in
ASTM D256
Vyncolit INSUL-PLATE™ X-28057-2HT Hole-Fill Powder For Printed Circuit Boards
Vyncolit INSUL-PLATE™ Hole-Fill material delivers true reliability and superior performance. This material, in powder form, is specifically suited for Hole-Fill use in glass epoxy, multi-layer and ..
Izod Impact, Notched 0.180 J/cm
<br>@Temperature 23.0 °C
0.337 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
LATI LARAMID CE/60 60% Mineral Filled Polyphthalamide (PPA) Based Compound &nbsp;(Unverified Data**)
Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s..
Izod Impact, Notched 0.180 - 0.267 J/cm
<br>@Temperature -20.0 - 0.000 °C
0.337 - 0.500 ft-lb/in
<br>@Temperature -4.00 - 32.0 °F
Average value: 0.215 J/cm Grade Count:4
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..
Copyright © lookpolymers.com All Rights Reserved