Polymer Property : Izod Impact, Notched = 0.200 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
ASTM D256
SABIC PP 519A Polypropylene Homopolymer for Spunbond Applications
Product Description: PP 519A is a controlled rheology grade with a narrow molecular weight distribution intended for spun bond fiber extrusion applications.PP 519A has the following features:Consis..
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
ASTM D256
SABIC PS 160 General Purpose Polystyrene for Foam Extrusion
Product Description: General purpose Polystyrene PS 160 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle material having High molecular ..
Izod Impact, Notched 0.200 - 0.300 J/cm
0.375 - 0.562 ft-lb/in
ASTM D256-06
Proto3000 Objet Digital Materials™ DM_Dots_7513 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t..
Izod Impact, Notched 0.200 - 0.300 J/cm
0.375 - 0.562 ft-lb/in
ASTM D256-06
Proto3000 Objet Digital Materials™ DM_Grid_7523 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t..
Izod Impact, Notched 0.200 - 0.300 J/cm
0.375 - 0.562 ft-lb/in
ASTM D256-06
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Izod Impact, Notched 0.200 - 0.300 J/cm
0.375 - 0.562 ft-lb/in
ASTM D256A
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer
WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look ..
Izod Impact, Notched 0.200 J/cm
<br>@Diameter 3.17 mm
0.375 ft-lb/in
<br>@Diameter 0.125 in
bar, 0.010&quot; notch radius; ASTM D256
Ineos Nova 2510 General Purpose Crystal Polystyrene &nbsp;(discontinued **)
High speed molding, Improved crack resistance, USP Class VIApplications: Cutlery, Light louvers, RazorsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phy..
Izod Impact, Notched 0.200 J/cm
<br>@Diameter 3.17 mm
0.375 ft-lb/in
<br>@Diameter 0.125 in
bar, 0.010&quot; notch radius; ASTM D256
Ineos Nova 2100 General Purpose Crystal Polystyrene &nbsp;(discontinued **)
Relative high heat resistance, Improved crack resistance, Good strengthApplications: Foam extrusion, Biaxially oriented sheet, Thermoforming applications, Molded packagingExposure to gamma radiation..
Izod Impact, Notched 0.200 - 0.300 J/cm
<br>@Diameter 3.17 mm
0.375 - 0.562 ft-lb/in
<br>@Diameter 0.125 in
bar
Ineos H00M-01 Polypropylene Homopolymer &nbsp;(discontinued **)
Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, High stiffness, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical application..
Izod Impact, Notched 0.200 J/cm
<br>@Temperature 23.0 °C
0.375 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
Flint Hills P9G8Z-036 Polypropylene Specialty Polypropylene
Features: Broad MWD Homopolymer. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion coatingInformation Provided by Flint Hills Resources
Izod Impact, Notched 0.200 J/cm
<br>@Diameter 3.17 mm
0.375 ft-lb/in
<br>@Diameter 0.125 in
bar, 0.010&quot; notch radius; ASTM D256
Ineos Nova 1504 High Heat Crystal Polystyrene
Good balance of flow, strength and set up properties, Blue edge effect, USP Class VIApplications: Consumer electronics, Housewares, Cosmetic packagingExposure to gamma radiation in the 2.02-6.06 meg..
Izod Impact, Notched 0.200 J/cm
<br>@Diameter 3.17 mm
0.375 ft-lb/in
<br>@Diameter 0.125 in
bar, 0.010&quot; notch radius; ASTM D256
Ineos Nova 1600 High Heat Crystal Polystyrene
High heat resistance, Moderate flow, Good balance of strength and set-upApplications: Foam extrusion, Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant e..
Izod Impact, Notched 0.200 - 0.300 J/cm
<br>@Diameter 3.17 mm
0.375 - 0.562 ft-lb/in
<br>@Diameter 0.125 in
bar; ASTM D256
Ineos H03G-00 Polypropylene Homopolymer
Suggested fabrication methods: ExtrusionFeatures: Low water carry-overTypical applications: Woven fabric, Cordage, Slit filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property d..
Izod Impact, Notched 0.200 - 0.300 J/cm
<br>@Diameter 3.17 mm
0.375 - 0.562 ft-lb/in
<br>@Diameter 0.125 in
bar; ASTM D256
Ineos H05A-00 Polypropylene Homopolymer
Grade H05A-00 is an antistatic polypropylene homopolymer for injection molding & extrusion applications. This material meeets the requirements of the U.S. Food and Drug Administration as specified ..
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
ASTM D882
Spartech Polycast SAR (Super Abrasion Resistant) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Izod Impact, Notched 0.200 J/cm
<br>@Thickness 3.20 mm
0.375 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Supreme Petrochem SC 203EL General Purpose Polystyrene
CharacteristicsMedium flow grade with good mechanical properties Improves productivity due to good balance of flow, heat and mold release propertiesProcessing Injection moldingApplicationsAudio cass..
Izod Impact, Notched 0.200 J/cm
<br>@Temperature 23.0 °C
0.375 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTASAN SAN 2000 Styrene Acrylonitrile
General purpose SANGood chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.200 - 0.220 J/cm
0.375 - 0.412 ft-lb/in
ASTM D256A
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons..
Izod Impact, Notched 0.200 - 0.300 J/cm
0.375 - 0.562 ft-lb/in
ASTM D256A
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless..
Izod Impact, Notched 0.200 J/cm
<br>@Temperature 23.0 °C
0.375 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256A
Braskem H 201 Injection Molding Polypropylene
Description: H 201 is a high melt flow rate additivated homopolymer suitable for injection molding and fiber extrusion applications. This product exhibits excellent processability with good melt sta..
Izod Impact, Notched 0.200 J/cm
<br>@Temperature 23.0 °C
0.375 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256A
Braskem H 502 HC Injection Molding Polypropylene
Description: H 502HC is a low melt flow rate homopolymer, designed for very high stiffness/toughness applications with good processability. This product exhibits excellent chemical resitance and bar..
Izod Impact, Notched 0.200 J/cm
<br>@Temperature 23.0 °C
0.375 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256A
Braskem H 117 Injection Molding Polypropylene
Description: H 117 is a ultra-high melt flow rate homopolymer. This product is suitable to high productivity on thin-walled parts. H 117 features an excellent stiffness, thermal resistance, low warp..
Izod Impact, Notched 0.200 J/cm
<br>@Diameter 3.17 mm
0.375 ft-lb/in
<br>@Diameter 0.125 in
bar, 0.010&quot; notch radius; ASTM D256
Ineos Nova 3511 General Purpose Crystal Polystyrene &nbsp;(discontinued **)
Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure..
Izod Impact, Notched 0.200 - 0.300 J/cm
<br>@Diameter 3.17 mm
0.375 - 0.562 ft-lb/in
<br>@Diameter 0.125 in
bar; ASTM D256
Ineos H14A-00 Polypropylene Homopolymer
Suggested fabrication methods: Injection molding and extrusion applications.Features: AntistaticTypical applications: Packaging, Closures, Consumer productsComplies with FDA specification, Title 21,..
Izod Impact, Notched 0.200 J/cm
<br>@Diameter 3.17 mm
0.375 ft-lb/in
<br>@Diameter 0.125 in
bar, 0.010&quot; notch radius; ISO 180
Ineos Nova 610 Crystal Polystyrene GP Grade &nbsp;(discontinued **)
Broad, medium melt flow range, Broad Vicat rangeApplications: Any; Injection Molding and ExtrusionProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise spe..
Izod Impact, Notched 0.200 J/cm
<br>@Diameter 3.17 mm
0.375 ft-lb/in
<br>@Diameter 0.125 in
bar, 0.010&quot; notch radius; ISO 180
Ineos Nova 205 Crystal Polystyrene General Purpose Grade &nbsp;(discontinued **)
Easy flow, Good mechanical property balance, Extrusion and Injection MoldingApplications: Sheet and film extrusion, Gloss capping, Blending with HIPS or SBSProperties were determined on injection m..
Izod Impact, Notched 0.200 J/cm
<br>@Diameter 3.17 mm
0.375 ft-lb/in
<br>@Diameter 0.125 in
bar, 0.010&quot; notch radius; ASTM D256
Ineos Nova 1200 High Heat Crystal Polystyrene
Good processing characteristics, High tensile strength and modulus, Excellent clarity, USP Class VIApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radia..
Izod Impact, Notched 0.200 - 0.300 J/cm
<br>@Diameter 3.17 mm
0.375 - 0.562 ft-lb/in
<br>@Diameter 0.125 in
bar; ASTM D256
BP Amoco Amoco® Polypropylene Homopolymer &nbsp;(discontinued **)
Suggested fabrication methods: Injection molding; Rotary CompressionFeatures: Nucleated, Antistatic, LubricatedTypical applications: Closures, CapsComplies with FDA specification, Title 21, CFR 177...
Izod Impact, Notched 0.200 - 0.300 J/cm
<br>@Diameter 3.17 mm
0.375 - 0.562 ft-lb/in
<br>@Diameter 0.125 in
bar; ASTM D256
Ineos H28U-00 Polypropylene Homopolymer &nbsp;(discontinued **)
Suggested fabrication methods: Injection moldingFeatures: Radiation stableTypical applications: MedicalComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject..
Izod Impact, Notched 0.200 - 0.300 J/cm
<br>@Diameter 3.17 mm
0.375 - 0.562 ft-lb/in
<br>@Diameter 0.125 in
bar; ASTM D256
Ineos H38K-00 Polypropylene Homopolymer, Fiber Grade &nbsp;(discontinued **)
Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fade, Low smokeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520..