Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.262 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.262 J/cm
0.491 ft-lb/in
Abatron AboCast 8-12/Abocure 8-12 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/13.2 ratio (pbw); Gel time, 100 g (3.5 oz.): 49 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F..
Izod Impact, Notched 0.262 J/cm
0.491 ft-lb/in
ASTM D256A
DSM Somos® 7110 Epoxy Photopolymer, Green Parts  (discontinued **)
DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u..
Izod Impact, Notched 0.262 J/cm
0.490 ft-lb/in
ASTM D256
Ensinger Tecatron® XP-84 Compression Molded PPS Compound, 30% Graphite Filled
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Izod Impact, Notched 0.262 J/cm
0.490 ft-lb/in
Atom Adhesives AA-SUPERTHERM 05 Epoxy Adhesive
AA-SUPERTHERM 05 is a thixotropic (smooth paste) Pure Diamond ultra-high thermally conductive epoxy two-part adhesive that develops strong, durable, high-impact bonds at room temperature which impro..
Izod Impact, Notched 0.262 J/cm

@Temperature 22.8 °C
0.490 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Teknor Apex Sinpolene CPP1040 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 40% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F..
Izod Impact, Notched 0.262 J/cm
0.490 ft-lb/in
Abatron AboCast/AboCure 7606-1 Epoxy
AboCast 7606-1 is a transparent, light amber resin with a weight of 9.5 lbs/gallon and a viscosity of 2100 cps approx. @ 25°C. AboCure 7606-1 is a transparent, light amber converter with a weight o..
Copyright © lookpolymers.com All Rights Reserved