| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in | 73°F; ASTM D256 |
|
Multibase Multi-Pro® 2006 T Polypropylene
Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Izod Impact, Notched |
0.374
J/cm <br>@Temperature 23.0 °C
|
0.700
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
RheTech Products CC40P100-00EG 40% Calcium Carbonate Reinforced Polypropylene, Natural, Extrusion Grade
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in | ASTM D256 |
|
Ravago Manufacturing Americas Hylon® N1240MHL BK Nylon 6/6
Available in North America Filler: Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated, Low Warpage and Heat StabilizedRoHS CompliantForm: Pellets Processing ..
|
|||
| Izod Impact, Notched |
0.374
J/cm <br>@Thickness 3.18 mm
|
0.701
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
LNP Emi-X® OC-1008 LEX Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **)
Features: Radio Frequency Shielding, Electromagnetic Shielding, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data ..
|
|||
| Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256 |
|
LNP NORYL® EXCP0111 PPS + Polyphenylene Ether, 42% Glass / Mineral Reinforcement
(discontinued **)
For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele..
|
|||
| Izod Impact, Notched | 0.374 - 4.21 J/cm | 0.700 - 7.89 ft-lb/in | Average value: 0.930 J/cm Grade Count:19 |
|
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
|
|||
| Izod Impact, Notched | 0.374 - 7.47 J/cm | 0.700 - 14.0 ft-lb/in | Average value: 1.94 J/cm Grade Count:22 |
|
Overview of materials for ABS/Polyester Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat..
|
|||
| Izod Impact, Notched |
0.374
J/cm <br>@Temperature 23.0 °C
|
0.700
ft-lb/in <br>@Temperature 73.4 °F
|
Method A; ASTM D256 |
|
Phillips 66 COPYLENE® CH085 Polypropylene, Homopolymer, Cast Film
COPYLENE™ CH085, a controlled rheology polypropylene homopolymer resin, is used in injection molding and cast film extrusion applications. Applications: Bags & Pouches, Stationery Film, Stretch Wra..
|
|||
| Izod Impact, Notched |
0.374
J/cm <br>@Thickness 3.17 mm
|
0.700
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES Electrablend® ABS CF10 FR BK 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched |
0.374
J/cm <br>@Thickness 3.17 mm
|
0.700
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES HiFill® PPS 0237 A
Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in | ASTM D256 |
|
Chase Plastics CP Pryme® NN100MD2 (DAM) Nylon 66 with 2% MoS2 Lubricated
Information provided by Chase Plastics.
|
|||
| Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256A |
|
Total PPH 3230 Polypropylene, Blow Molding Grade
Homopolymer blow molding gradeLubricated - Fina 3230 offers superior core rod release, eliminating the need for additional lubricant.High Purity - Fina 3230 features minimum taste and odor and optim..
|
|||
| Izod Impact, Notched |
0.374
J/cm <br>@Thickness 3.17 mm
|
0.700
ft-lb/in <br>@Thickness 0.125 in
|
injection molded sample; ASTM D256 |
|
American Polymers API 410 Polystyrene
API 410 is a low impact polystyrene with very high gloss and superior dimensional stability.Applications: API 410 is ideally suited for point of purchase displays where high gloss and some impact i..
|
|||
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in | ASTM D256 |
|
Ensinger HYDEX® 4101 Polybutylene Terephthalate (PBT)
HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for ma..
|
|||
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in | ASTM D256 |
|
Ensinger Tecapeek® XP-181 Compression Molded PPEK Compound, EWS Filled and Carbon Fiber Reinforced
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
|
|||
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in | ASTM D256A |
|
Braskem D042M Homopolymer Polypropylene
Description: Injection Molding, General Purpose, Low Water Carryover, UV ResistantApplications: Suggested Uses Include Tape, Slit-film Fibers, Containers, Closures, HousewaresThis resin meets the re..
|
|||
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in | ASTM D256A |
|
Braskem FT200WV Homopolymer Polypropylene
Description: Good mold release, nucleated, excellent rigidity and hardness.Applications: Suggested uses include housewares, caps and closures, fast-cycle injection molding.Process: Injection Molding..
|
|||
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in | ASTM D256A |
|
Braskem TI71200M High Crystallinity Copolymer Polypropylene
Description: Highly crystalline homopolymer phase, very high molecular weight EPR phase, very high flexural modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding...
|
|||
| Izod Impact, Notched | 0.374 - 5340 J/cm | 0.700 - 10000 ft-lb/in | Average value: 1.46 J/cm Grade Count:180 |
|
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
|
|||
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in | ASTM D256 |
|
Asahi Kasei Thermofil P-10CC-Y488 10% Calcium Carbonate Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256 |
|
LNP ULTEM® SMU5832 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **)
ESD characteristics for ultra high-heat applications. Will be UC3010.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compan..
|
|||
| Izod Impact, Notched | 0.374 - 0.747 J/cm | 0.700 - 1.40 ft-lb/in | Average value: 0.587 J/cm Grade Count:10 |
|
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
|
|||
| Izod Impact, Notched | 0.374 - 0.908 J/cm | 0.700 - 1.70 ft-lb/in | Average value: 0.662 J/cm Grade Count:25 |
|
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi..
|
|||