| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP FARADEX PS003E PA 6
LNP* FARADEX* PS003E is a compound based on Nylon 6 resin containing 15% Stainless Steel. Added features of this material include: EMI/RFI Shielding.
|
|||
| Izod Impact, Notched | 0.420 - 1.28 J/cm | 0.787 - 2.40 ft-lb/in | Average value: 0.679 J/cm Grade Count:53 |
|
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
|
|||
| Izod Impact, Notched |
0.420
J/cm @Temperature 23.0 °C |
0.787
ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
|
IRPC Polimaxx Polene 3342M Polypropylene Random Copolymer
CHARACTERISTICS: HIGH CLARITY, GOOD FLOW, GOOD PROCESSABILITY APPLICATIONS: INJECTION MOLDING, INJECTION STRETCH BLOW MOLDING (ISBM) FOR FOOD CONTAINERS, BOTTLES, HOUSEWARES, CRATES
|
|||
| Izod Impact, Notched |
0.420
J/cm @Temperature 23.0 °C |
0.787
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Lubricomp FFL21 PE
LNP* Lubricomp* FFL21 is a compound based on Polyethylene resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for t..
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA 6/12 (Asia Pacific)
LNP* Lubricomp* IAL12 is a compound based on Nylon 6/12 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated.
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRICOMP KFL32R Acetal Copolymer
LNP LUBRICOMP* KFL32R is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE. Added feature of this material is: Easy Release, Wear Resistant.
|
|||
| Izod Impact, Notched |
0.420
J/cm @Temperature 23.0 °C |
0.787
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer
LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f..
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL003 Acetal Copolymer (Asia Pacific)
LNP* LUBRICOMP* KL003 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Europe-Africa-Middle East)
LNP* LUBRICOMP* KL004 is a compound based on Acetal Copolymer containing PTFE. Added features include Internally Lubricated.
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer
LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized.
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66
LNP LUBRICOMP* RL004S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant.
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP STAT-KON AX06518 ABS (Asia Pacific)
LNP* Stat-kon* AX06518 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, Fl..
|
|||
| Izod Impact, Notched |
0.420
J/cm @Temperature 23.0 °C |
0.787
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East)
DATA ON BK1005 ONLY.
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP STAT-KON Noryl_NC3508 PPE+HIPS (Europe-Africa-Middle East)
PRELIMINARY DATA. LNP* Stat-kon* Noryl_NC3508 compound is a 33% glass/mineral/carbon filled PPE+PS. ESD, high heat, tight tolerance: electronic packaging/chip trays.
|
|||
| Izod Impact, Notched |
0.420
J/cm @Temperature 23.0 °C |
0.787
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Stat-kon RX89129 PA 66
LNP* Stat-Kon RX89129 is a compound based on Nylon 6,6. Fillers are proprietary.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched |
0.420
J/cm @Temperature 23.0 °C |
0.787
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Thermocomp RFZ71S PA 66
LNP* Thermocomp* RFZ71S is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for t..
|
|||
| Izod Impact, Notched |
0.420
J/cm @Temperature 23.0 °C |
0.787
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Thermocomp RFZ71S PA 66 (Asia Pacific)
LNP* Thermocomp* RFZ71S is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for t..
|
|||
| Izod Impact, Notched |
0.420
J/cm @Temperature 23.0 °C |
0.787
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly
LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP DB008ERP PC (Asia Pacific)
LNP* Thermocomp* DB008ERP is a compound based on Polycarbonate resin containing Glass Bead. Added features of this material include: Easy Molding, Mold Release.
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP PF001S PA 6
LNP* THERMOCOMP* PF001S is a compound based on Nylon 6 resin containing 5% Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP WF006U PBT
LNP* THERMOCOMP* WF006U is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this material is: UV Stabilized.
|
|||
| Izod Impact, Notched |
0.420
J/cm @Temperature 23.0 °C |
0.787
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Thermotuf VFM53 PA 66
LNP THERMOTUF* VFM53 is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas..
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ FPP 3715 Glass Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 3715 is a 15% glass filled homopolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256A |
|
Total PPH 3281 Polypropylene, Extrusion Grade
Low melt flow homopolymer for sheet extrusion, strapping, and in-line thermoforming applicationsMelt Strength – The high melt strength of FINA 3281 allows uniform drawdown during processing, result..
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ FPP 3715 Glass Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 3715 is a 15% glass filled homopolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 0.420 - 0.881 J/cm | 0.787 - 1.65 ft-lb/in | Average value: 0.638 J/cm Grade Count:34 |
|
Overview of materials for Acetal Copolymer + Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of ..
|
|||
| Izod Impact, Notched |
0.420
J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
0.787
ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
|
Premix Thermoplastics PRE-ELEC® 12-034
(discontinued **)
PRE-ELEC 12-034 is a conductive thermoplastic compound based on a polyacetal copolymer with 40% carbon fiber. PRE-ELEC 12-034 exhibits excellent mechanical properties and electrical conductivity. Te..
|
|||
| Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP AX06472 ABS
LNP* Thermocomp* AX06472 is a compound based on ABS containing a clay blend.
|
|||